What Is Galvalume? ASTM A792 Coated Steel Explained

Galvalume is sheet steel with a 55% aluminum-zinc alloy coating. Learn how ASTM A792 AZ designations work, why it lasts on roofs, and where it should not be used.

Updated October 2026 5 min read By the ASA team

On this page
  1. How the aluminum-zinc coating works
  2. ASTM A792 AZ coating designations
  3. Where Galvalume performs best
  4. Limitations and compatibility rules
  5. Fabricating Galvalume
  6. Galvalume from ASA

Galvalume is sheet steel hot-dip coated with an alloy of about 55% aluminum, 43.4% zinc and 1.6% silicon by weight, made to ASTM A792. The aluminum gives a durable barrier that weathers slowly, while the zinc adds sacrificial protection at scratches and cut edges, so Galvalume typically outlasts galvanized sheet of similar coating thickness in outdoor atmospheric exposure.

Galvalume is a trademarked name; the generic term is 55% aluminum-zinc alloy coated steel. It is the dominant substrate for unpainted and prepainted metal roofing and wall panels, and it shows up in equipment housings and building trim that must last for decades with little maintenance.

How the aluminum-zinc coating works

As the coating solidifies, it forms aluminum-rich dendrites with zinc-rich material filling the spaces between them. The two parts do different jobs:

  • Aluminum-rich regions form a tough, stable oxide that corrodes very slowly in air. This barrier is where most of Galvalume’s long life comes from.
  • Zinc-rich regions corrode preferentially and protect exposed steel at cut edges and scratches, the way galvanized coating does, though to a lesser degree.
  • Silicon (about 1.6%) controls the growth of the brittle iron-aluminum alloy layer next to the steel, so the coating stays adherent and formable.

The result is a coating that sits between pure zinc and pure aluminum. It wears away much more slowly than zinc in most atmospheres, but it gives less galvanic protection at edges than galvanized because the zinc fraction is smaller.

ASTM A792 AZ coating designations

ASTM A792 uses “AZ” designations that follow the same logic as galvanized “G” designations: the number is the minimum total coating weight on both sides, in hundredths of an ounce per square foot, by the triple spot test. AZ50 means at least 0.50 oz/ft² total.

Because the aluminum-zinc alloy is roughly half as dense as zinc, the same weight of coating is about twice as thick. The table shows approximate thickness at each triple spot minimum, calculated from the coating weight using a density of 3.75 g/cm³ for the alloy and an even split between sides.

DesignationMin total, triple spotMin total, single spotApprox thickness per sideTypical use
AZ400.40 oz/ft²0.35 oz/ft²0.64 mil (16 µm)Lighter coating for painted or sheltered parts
AZ500.50 oz/ft²0.43 oz/ft²0.80 mil (20 µm)Prepainted roofing and wall panels
AZ550.55 oz/ft²0.50 oz/ft²0.88 mil (22 µm)Unpainted roofing and siding

For comparison, G90 galvanized carries about 0.76 mil (19 µm) of zinc per side. AZ55 therefore has a slightly thicker coating than G90 despite its lower weight, and its alloy corrodes more slowly. Unlike A653, A792 sets no triple spot minimum for each side. Metric editions use AZM designations in grams per square meter; AZM120, AZM150 and AZM165 correspond to AZ40, AZ50 and AZ55.

Base steel designations

Like ASTM A653, A792 also defines the steel under the coating: Commercial Steel (CS), Forming Steel (FS), and Structural Steel (SS) in several grades with guaranteed yield and tensile minimums. Thin roofing panels are often rolled from high strength structural grades, while bent trim and flashing usually use CS. A full order names all three pieces: specification, designation and coating, for example ASTM A792 CS Type B, AZ50.

Where Galvalume performs best

Galvalume’s strength is long service in the open atmosphere, especially where surfaces drain and dry between wettings. Typical applications include:

  • Standing seam and through-fastened metal roofing
  • Wall panels, siding, soffits and liner panels
  • Gutters, downspouts, flashing and trim
  • Garage doors and agricultural and industrial building skins
  • HVAC housings, outdoor equipment cabinets and enclosure skins
  • Appliance parts where heat reflectivity and a bright surface matter

Galvalume reflects heat better than weathered galvanized and holds a bright, spangled appearance for years. Most sheet is supplied with a thin clear acrylic or similar treatment that resists fingerprints, handling marks and wet storage stain during shipping and installation.

Limitations and compatibility rules

Aluminum changes how the coating reacts with its surroundings. Several contact conditions that galvanized sheet tolerates can damage Galvalume:

  • Wet concrete and mortar: fresh concrete is strongly alkaline and attacks aluminum. Keep Galvalume out of direct contact with wet concrete, mortar and plaster.
  • Animal confinement buildings: ammonia and moisture from livestock waste attack the coating. Producers generally do not recommend bare Galvalume for these interiors.
  • Copper and lead: direct contact, or water running off copper or lead onto the panel, causes accelerated corrosion. Use compatible flashing and fasteners.
  • Cut edges on heavier gauges: with less zinc available, thick sheet may show light edge rust staining. On thin panels this is usually cosmetic and self-limiting.
  • Graphite pencils: graphite marks on aluminum-zinc and zinc coatings can cause local corrosion. Mark with a felt marker instead.

Tip: When Galvalume panels will sit on or near masonry or a concrete slab, specify a barrier such as a membrane or keep the panels above the slab line. Most early failures come from contact, not from the weather.

Fabricating Galvalume

Galvalume roll forms, brakes and shears well. The coating is somewhat harder than zinc, so it resists scuffing in forming tools, but very tight bends on heavy coatings can show fine crazing at the outside of the bend, which normally does not affect performance.

It can be resistance welded and arc welded, though the aluminum in the coating changes welding behavior. Resistance welding settings differ from those for galvanized and are best confirmed with trial welds, and arc welding still produces zinc fume and needs extraction. Many Galvalume products are joined mechanically with fasteners, clinching or seaming rather than welding.

Store bundles dry, under cover and slightly inclined so water drains. Moisture trapped between sheets causes wet storage stain, which on Galvalume shows up as dark gray or black staining rather than the white powder seen on galvanized. Light staining is mostly cosmetic, but prolonged trapped moisture consumes coating, so separate and dry any sheets that get wet in transit. Handle visible panels with clean gloves and lift sheets rather than sliding them, which avoids fingerprints and scuffs that show on the bright surface for years.

Galvalume takes coil-applied paint systems very well, and prepainted Galvalume is standard for colored roof and wall panels. Field painting is possible with a primer rated for aluminum-zinc coatings after cleaning off any surface treatment.

To see how it stacks up against zinc and zinc-iron coatings on cost, paint, welding and edge protection, read galvanized vs galvannealed vs Galvalume, or the basics in what galvanized steel is.

Galvalume from ASA

ASA’s stock list includes Galvalume to ASTM A792 AZ40 in its flat-rolled sheet and plate line, with mill certifications and full material traceability available. Coated sheet from 24 to 11 gauge can be leveled and cut to length on ASA’s leveling and cut-to-length line, with PVC film or interleaving to protect the surface, then laser cut and formed in house. Call 1-800-933-7833 to discuss coating weight and designation for your parts.

Frequently asked questions

Is Galvalume better than galvanized steel?

For long atmospheric exposure such as roofs and walls, Galvalume usually lasts longer because its aluminum-rich coating weathers more slowly than zinc. Galvanized is better where strong cut-edge protection, contact with concrete, or animal confinement exposure is involved, and it is easier to weld. The better choice depends on the environment and how the part will be fabricated.

Is Galvalume the same as aluminized steel?

No. Galvalume carries an alloy of about 55% aluminum and 43% zinc under ASTM A792. Aluminized steel carries an aluminum or aluminum-silicon coating with no zinc under ASTM A463. Aluminized steel is chosen mainly for heat resistance in exhaust and oven parts, while Galvalume is chosen for long-lived roofing and siding.

Can Galvalume touch treated lumber?

Contact with wet, preservative-treated lumber is a concern for most metal coatings, because some treatments contain copper compounds that accelerate corrosion. Producers generally advise a barrier, such as an underlayment or membrane, between Galvalume panels and treated wood. Check the panel manufacturer's installation guidance and the lumber treatment type before installation.

What does AZ55 mean?

AZ55 is an ASTM A792 coating designation meaning at least 0.55 ounces of aluminum-zinc alloy per square foot of sheet, both sides combined, by the triple spot test. It works out to roughly 0.88 mil of coating per side. AZ55 is the weight most often specified for unpainted Galvalume roofing and siding panels.

Does Galvalume rust at screw holes and cut edges?

Cut edges and screw holes expose bare steel, and Galvalume protects them less aggressively than zinc. On thin roofing panels, edges may show slight staining that typically stops as corrosion products seal the edge. On thicker sheet or in wet, salty sites, edge rust can be more noticeable, so edge sealing or a painted product is worth considering.

Material, processing and fabrication from one supplier

Send a drawing or a material list and the ASA team will quote it from stock.