ASTM B209: Aluminum Sheet and Plate Specification

What ASTM B209 covers, how aluminum alloy and temper designations work, key property limits for 3003 and 5052, and how to write the order.

Updated October 2026 5 min read By the ASA team

On this page
  1. What ASTM B209 covers
  2. Alloy and temper designations
  3. Mechanical properties of common alloys
  4. Tolerances, finish and certification
  5. B209, SB-209 and aerospace specifications
  6. What to write on a purchase order
  7. Buying B209 aluminum from ASA

ASTM B209 is the standard specification for aluminum and aluminum-alloy flat sheet, coiled sheet and plate. It sets the chemical composition, mechanical property limits by alloy, temper and thickness, and the testing and certification rules for wrought aluminum flat products such as 3003, 5005 and 5052. Most commercial aluminum sheet and plate in the US is bought and certified to B209.

B209 values are specified as a range or minimum for each combination of alloy, temper and thickness, so the alloy alone does not define the material. A complete callout names all three, for example ASTM B209, 5052-H32, 0.125 in.

What ASTM B209 covers

B209 covers both non-heat-treatable alloys, which gain strength by cold working (the 1xxx, 3xxx and 5xxx series), and heat-treatable alloys, which gain strength by solution heat treatment and aging (the 2xxx and 7xxx series, among others). It also covers alclad products, in which the core alloy is clad with a thin surface layer of aluminum or an aluminum alloy that protects the core from corrosion.

The product forms are defined by thickness:

ProductThickness
FoilUnder 0.006 in (0.15 mm)
Sheet0.006 to 0.249 in (0.15 to 6.32 mm)
Plate0.250 in (6.35 mm) and thicker

Unlike steel, aluminum sheet is almost always ordered by decimal thickness rather than gauge. Extrusions, bar and rod are covered by other specifications, such as ASTM B221, and are not part of B209. Dimensional tolerances for B209 products are taken from ANSI H35.2, the American National Standard for dimensional tolerances of aluminum mill products.

Alloy and temper designations

Aluminum alloys use the four-digit system registered with the Aluminum Association, and tempers follow ANSI H35.1. The temper suffix tells you how the material was strengthened and roughly how hard it is. For strain hardened tempers, the second digit indicates hardness: 2 is quarter hard, 4 is half hard, 6 is three-quarter hard and 8 is full hard.

TemperMeaningExample
OAnnealed, softest condition5052-O for severe forming
H1xStrain hardened only3003-H14 (half hard)
H2xStrain hardened, then partially annealed3003-H22
H3xStrain hardened, then stabilized by low-temperature heating5052-H32 (quarter hard), 5052-H34 (half hard)
THeat treated to a stable temper2024-T3, 7075-T6 (heat-treatable alloys)

The difference between H1x and H3x matters for 5xxx alloys. Magnesium-bearing alloys can soften slowly at room temperature after cold working, so they are stabilized by a low-temperature heat treatment. That is why 5052 is most often sold as H32 and H34.

Chemistry of common B209 sheet alloys

AlloyMain alloying element(s)Character
3003Manganese 1.0 to 1.5%, copper 0.05 to 0.20%General purpose, very formable, moderate strength
5005Magnesium 0.50 to 1.1%Similar strength to 3003, good anodizing response
5052Magnesium 2.2 to 2.8%, chromium 0.15 to 0.35%Higher strength, good corrosion resistance in marine air

Each alloy also has maximum limits for iron, silicon, zinc and other elements, and aluminum makes up the remainder. The guides to 3003-H14 aluminum and 5052 aluminum cover how these alloys behave in fabrication.

Mechanical properties of common alloys

B209 lists tensile strength as a range for most strain hardened tempers, with a minimum yield strength and a minimum elongation that varies with thickness. These are the limits for the typical sheet thickness range:

Alloy and temperTensile strengthYield strength, min
3003-H1420.0 to 26.0 ksi (140 to 180 MPa)17.0 ksi (115 MPa)
5052-H3231.0 to 38.0 ksi (215 to 265 MPa)23.0 ksi (160 MPa)
5052-H3434.0 to 41.0 ksi (235 to 285 MPa)26.0 ksi (180 MPa)

Notice that tensile strength has a maximum as well as a minimum. That upper limit helps protect formability, since sheet that is too hard for its temper is more likely to crack in bending. 5052-H32 has a minimum yield about 35% higher than 3003-H14 and a minimum tensile about 55% higher, and it still bends well, which makes it the usual upgrade when a 3003 part needs more stiffness or will see salt air.

Tip: When a part is bent tightly, check the minimum bend radius for the alloy and temper, not just the alloy. 5052-H32 tolerates tighter bends than 5052-H34, and O temper bends tightest of all.

Temper also changes with heat. Welding anneals strain hardened alloys such as 3003 and 5052 in the heat-affected zone, so the metal next to a weld drops back toward O temper strength. Welded designs in these alloys are normally checked against annealed properties, whatever temper was ordered.

Tolerances, finish and certification

Standard B209 product is mill finish: the surface as it leaves the rolling mill, clean but with no specified appearance. Surfaces for decorative, anodized or painted parts should be called out on the order, as should protective film or paper interleaving for polished or bright sheet. Flatness, thickness, width and length tolerances follow ANSI H35.2 unless the order specifies something tighter.

Store B209 sheet dry and off the floor. Water trapped between stacked sheets, often from condensation after a cold delivery, leaves white or gray water stain that does not polish out easily and can show through anodizing.

Mechanical properties are verified by tension tests on each lot, and the producer certifies conformance on a mill test report showing the alloy, temper, chemistry and test results. For pressure equipment built to the ASME Boiler and Pressure Vessel Code, the matching specification is ASME SB-209, which follows B209 requirements.

B209, SB-209 and aerospace specifications

Some drawings call for aerospace material specifications instead of, or as well as, B209. SAE’s AMS 4015, AMS 4016 and AMS 4017 cover 5052 sheet and plate in the O, H32 and H34 tempers respectively, and AMS-QQ-A-250 detail specifications replaced the old federal QQ-A-250 series for defense and aerospace plate and sheet. The guide to AMS-QQ-A-250 explains those documents. When a drawing names an AMS or military specification, material certified only to B209 is not a substitute unless the customer approves it.

What to write on a purchase order

  • ASTM B209 (or B209M), or ASME SB-209, and the edition if your quality system requires it
  • Alloy and temper, for example 5052-H32
  • Thickness as a decimal, width and length, or coil
  • Finish (mill finish unless stated), and PVC film or paper interleaving if needed
  • Any tolerance or flatness requirement tighter than standard
  • Mill test report and quantity

Example: ASTM B209, 5052-H32 aluminum sheet, 0.090 x 48 x 144 in, mill finish, paper interleaved, mill test report required. To estimate shipping weight, use the aluminum sheet and plate weight chart.

Buying B209 aluminum from ASA

American Steel & Aluminum stocks aluminum sheet in 3003-H14, 5005 and 5052-H32/H34, with ASTM B209, ASME SB-209, AMS 4015, 4016 and 4017 and AMS-QQ-A-250/8 on its stock list. ASA certifies 3003 to ASTM B209, which replaced the cancelled AMS-QQ-A-250/2. ASA levels and cuts aluminum from 0.032 to 0.125 in thick and cuts parts on an 8 kW fiber laser. Request a quote with alloy, temper, thickness and quantity.

Frequently asked questions

When does aluminum sheet become plate under ASTM B209?

Aluminum is classed as plate at 0.250 in (6.35 mm) thick and above. Sheet runs from 0.006 in to 0.249 in, and anything thinner is foil. Both sheet and plate are covered by B209, but mechanical property limits change across thickness ranges, so the exact thickness belongs on the order with the alloy and temper.

What is the difference between 5052-H32 and 5052-H34?

Both are strain hardened and stabilized. H32 is quarter hard and H34 is half hard. Under B209, H32 has a tensile range of 31.0 to 38.0 ksi and H34 a range of 34.0 to 41.0 ksi, with minimum yield of 23.0 and 26.0 ksi. H32 bends more easily; H34 is stiffer and resists denting slightly better.

Is ASTM B209 the same as ASME SB-209?

SB-209 is ASME's version of B209 for use under the Boiler and Pressure Vessel Code, and it follows the same requirements. Code-stamped equipment needs material certified to SB-209. For general fabrication, B209 is the usual callout, and mill test reports for flat aluminum often list both specifications so the same stock can serve either use.

Does ASTM B209 cover aluminum extrusions?

No. B209 is limited to flat-rolled sheet, coiled sheet and plate. Extruded bar, rod, shapes and tube are covered by ASTM B221, and other product forms have their own specifications. When an assembly combines sheet and extrusions, each part should reference its own specification on the drawing and purchase order.

Material, processing and fabrication from one supplier