ASTM A240 is the standard specification for chromium, chromium-nickel and chromium-manganese-nickel stainless steel plate, sheet and strip for pressure vessels and for general applications. It sets the chemical composition and the minimum mechanical properties for each stainless grade it lists, including 304, 304L, 316, 316L and 430, and it is the specification most US buyers cite for flat-rolled stainless.
A240 works as a pair with ASTM A480, which carries the general requirements: dimensional and flatness tolerances, surface finishes, test methods and certification. ASME SA240 and SA480 are the Boiler and Pressure Vessel Code versions used for code-stamped equipment.
What ASTM A240 covers
A240 covers flat-rolled stainless steel in all four of the main families: austenitic grades such as 304 and 316, ferritic grades such as 430 and 409, martensitic grades such as 410, and duplex grades such as 2205. Each grade is listed by its UNS number with its own chemistry limits and mechanical property requirements.
Despite the words “pressure vessels” in its title, A240 is used far beyond tanks and boilers. Enclosures, food equipment, architectural panels and machine guards made from stainless sheet are routinely bought to A240, because it is the specification mills certify flat stainless to. Stainless bar and structural shapes are covered by other specifications, such as ASTM A276 and A479, and ASTM A666 covers annealed and cold-worked austenitic stainless for structural uses that need higher strength.
The split between product forms follows A480. Material 3/16 in (4.76 mm) and thicker is generally plate; thinner material is sheet or strip depending on width. The same grade requirements in A240 apply to all three.
Chemistry of common A240 grades
The table shows key limits in weight percent for the grades most often ordered from a service center. All five also have limits on manganese, silicon, phosphorus, sulfur and, for the austenitic grades, nitrogen.
| Grade (UNS) | Carbon, max | Chromium | Nickel | Molybdenum |
|---|---|---|---|---|
| 304 (S30400) | 0.07 | 17.5 to 19.5 | 8.0 to 10.5 | None |
| 304L (S30403) | 0.030 | 17.5 to 19.5 | 8.0 to 12.0 | None |
| 316 (S31600) | 0.08 | 16.0 to 18.0 | 10.0 to 14.0 | 2.00 to 3.00 |
| 316L (S31603) | 0.030 | 16.0 to 18.0 | 10.0 to 14.0 | 2.00 to 3.00 |
| 430 (S43000) | 0.12 | 16.0 to 18.0 | 0.75 max | None |
Three differences drive most grade choices. The L grades cut carbon to 0.030% to prevent sensitization when heavy sections are welded. Molybdenum in 316 and 316L improves resistance to chlorides. And 430 drops nickel almost entirely, which makes it ferritic, magnetic and lower in cost, with less corrosion resistance and formability than 304. The guide on how to choose a stainless steel grade walks through those trade-offs.
Mechanical property requirements
A240 sets minimum strength and elongation, plus a maximum hardness, for each grade in the annealed condition. Mill test reports normally show measured values above these minimums.
| Grade | Tensile, min | Yield (0.2% offset), min | Elongation in 2 in, min | Hardness, max |
|---|---|---|---|---|
| 304 | 75 ksi (515 MPa) | 30 ksi (205 MPa) | 40% | 92 HRB (201 HBW) |
| 304L | 70 ksi (485 MPa) | 25 ksi (170 MPa) | 40% | 92 HRB (201 HBW) |
| 316 | 75 ksi (515 MPa) | 30 ksi (205 MPa) | 40% | 95 HRB (217 HBW) |
| 316L | 70 ksi (485 MPa) | 25 ksi (170 MPa) | 40% | 95 HRB (217 HBW) |
| 430 | 65 ksi (450 MPa) | 30 ksi (205 MPa) | 22% | 89 HRB (183 HBW) |
The L grades carry minimums 5 ksi lower than their standard counterparts because carbon adds strength to austenitic stainless. That gap is the reason dual certification exists. Material that meets the 0.030% carbon limit of 304L and the strength minimums of 304 can be certified to both grades on one mill report, and much of the 304L and 316L plate and sheet on the market today is sold that way.
Reading an A240 mill test report
Because 304, 316 and their L versions look identical, the mill test report is the practical proof of grade. Check that it names the specification and edition, the grade or grades certified, and a heat number that matches the marking on the material. The chemistry should fall inside the limits above, with carbon at or below 0.030% for any L grade and molybdenum present for 316. Tensile, yield, elongation and hardness should meet the table. Where a contract restricts melt origin, the report or a separate statement should also show where the steel was melted.
For grade-level detail, see the guides to 304 stainless steel and 430 stainless steel.
Finishes under ASTM A480
A240 does not set the surface finish; the order does, using the finish designations defined in ASTM A480. The most common ones for sheet and plate are:
| Finish | How it is made | Typical use |
|---|---|---|
| No. 1 | Hot rolled, annealed and descaled | Plate and heavy sections where appearance does not matter |
| 2D | Cold rolled, annealed and descaled; dull | Deep drawn parts, surfaces that will be finished later |
| 2B | Cold rolled, annealed, descaled, then lightly rolled on polished rolls | The general-purpose sheet finish for fabrication |
| BA | Cold rolled and bright annealed in a controlled atmosphere | Reflective trim, appliance and decorative parts |
| No. 4 | Polished with abrasive to a directional grain | Visible panels, food equipment, architectural work |
Finish affects more than appearance. Smoother finishes such as 2B, BA and No. 4 are easier to clean and hold less dirt and salt residue, which improves real-world corrosion performance. Polished finishes are directional, so the grain direction belongs on the drawing for visible parts, and many buyers order polished or bright sheet with a protective PVC film.
Tip: For laser cut parts with visible faces, specify PVC-coated sheet and state which side the film should be on. The film protects the finish through cutting, forming and handling.
A240, SA240 and what to put on the order
ASME SA240 is adopted from ASTM A240 for use under the Boiler and Pressure Vessel Code. For code work, the mill report must show SA240; for general fabrication, A240 is sufficient. Many mill reports list both, along with A480 and SA480.
A complete stainless order or RFQ includes:
- Specification: ASTM A240/A480, or ASME SA240/SA480 for code work
- Grade and UNS number, and whether dual certification is acceptable or required
- Product form and finish (for example 2B sheet or No. 1 plate)
- Thickness as a decimal, width and length
- Protective film or paper interleaving, if needed
- Mill test report, and any domestic melt or DFARS documentation the contract requires
- Quantity and processing (cut to size, laser cut, formed)
Example: ASTM A240/A480, Type 304/304L dual certified, 2B finish, 0.0625 x 48 x 120 in, PVC one side, mill test report required.
Buying A240 stainless from ASA
American Steel & Aluminum stocks 304, 304L, 316, 316L and 430 stainless, with 430 in 2B and BA finishes, and its stock list references ASTM A240, A480 and A666 and ASME SA240/SA480. ASA levels stainless from 24 to 10 gauge with PVC and interleaving options, cuts parts on an 8 kW fiber laser, and provides mill certifications with full traceability. Request a quote with grade, finish and size.
Frequently asked questions
Is ASTM A240 the same as ASME SA240?
SA240 is ASME's adoption of ASTM A240 for the Boiler and Pressure Vessel Code, and its requirements are essentially the same. The difference is which document the job calls for. Code-stamped pressure equipment requires material certified to SA240, while general fabrication can use A240. Many mills certify flat stainless to both on a single report.
Does ASTM A240 cover stainless steel bar?
No. A240 is limited to flat-rolled plate, sheet and strip. Stainless bars and shapes are covered by other ASTM specifications, such as A276 for general bars and A479 for bars used in boilers and pressure vessels. Name the correct specification for each product form on a mixed order so the mill reports match.
What does dual certified 304/304L mean?
Dual certified material meets the requirements of both grades at once: carbon at or below the 0.030% limit for 304L, and tensile and yield strength at or above the higher minimums for 304. One mill report lists both grades. It lets a fabricator stock a single material for drawings that call for either grade.
Which finish should I order for A240 stainless sheet?
2B is the standard cold rolled finish for general fabrication: smooth, moderately reflective and easy to clean. BA is brighter and suits decorative parts. No. 4 is a brushed, directional finish common on visible panels and food equipment. Heavier plate is usually No. 1. The finish is defined in ASTM A480 and must be stated on the order.