On this page
ASTM A1018 is the standard specification for hot rolled, heavy-thickness steel coils: sheet and strip from 0.230 in through 1.000 in (6.0 to 25 mm) thick that is produced and sold in coil form. It picks up where ASTM A1011 stops and covers commercial, drawing, structural, high-strength low-alloy, improved formability and ultra-high strength steels.
The key rule for buyers is that A1018 material is meant to be fed from the coil into blanking, forming, drawing, rolling or a tube mill. It cannot be sold as structural or pressure vessel plate unless it is tested to the plate rules in ASTM A6 or A20. That one clause explains most of the confusion between coil-processed material and plate.
What ASTM A1018 covers
A1018 applies to hot rolled coils beyond the size limits of ASTM A1011. The size range is set by thickness and width:
| Product | Thickness | Width |
|---|---|---|
| Heavy-thickness strip (coil) | 0.230 to 1.000 in (6.0 to 25 mm) | Over 8 to 12 in (over 200 to 300 mm) |
| Heavy-thickness sheet (coil) | 0.230 to 1.000 in (6.0 to 25 mm) | Over 12 in (over 300 mm) |
Hot rolled material in these thicknesses would normally be called plate if it were rolled as individual pieces. Modern hot strip mills can coil it instead, which makes it efficient to slit, blank and form at high volume. A1018 gives that coiled product its own rules for chemistry, testing and designation.
Dimensional tolerances for A1018 material come from ASTM A635, the general requirements specification for heavy-thickness hot rolled coils.
Designations in A1018
| Designation | Grades, types or classes | What is guaranteed |
|---|---|---|
| Commercial Steel (CS) | Types A and B, or a standard steel chemistry | Chemistry |
| Drawing Steel (DS) | Types A and B, or a standard steel chemistry | Chemistry |
| Structural Steel (SS) | Grades 30, 33, 36 (Types 1 and 2) and 40 | Chemistry plus minimum strength |
| High-Strength Low-Alloy (HSLAS) | Grades 45 to 70, Classes 1 and 2 | Chemistry plus minimum strength |
| HSLAS with Improved Formability (HSLAS-F) | Grades 50, 60, 70 and 80 | Chemistry plus minimum strength |
| Ultra-High Strength Steel (UHSS) | Grades 90 and 100, Types 1 and 2 | Chemistry plus minimum strength |
The designations follow the same logic as the lighter sheet specifications. CS and DS are bought for formability and are controlled by chemistry; the SS, HSLAS, HSLAS-F and UHSS designations carry mandatory minimum yield and tensile strength, and the grade number is the minimum yield in ksi. HSLAS is offered in two classes, with Class 2 aimed at better formability.
SS Grade 36 comes in two types. Type 2 is the variant aligned with A36 strength, with a 36 ksi (250 MPa) minimum yield and a 58 ksi (400 MPa) minimum tensile strength (confirm the exact tensile requirement in the edition you order to), in line with the minimums of A36 steel. If a drawing calls for A36 properties on a part blanked from heavy coil, A1018 SS Grade 36 Type 2 is the designation to discuss with your supplier, with the plate conversion rule below in mind.
For the higher strength options, HSLA steel explains how microalloyed grades reach their strength with low carbon, which helps both weldability and forming.
Coil-processed material vs plate
| Point | A1011 sheet and strip | A1018 heavy coil | Plate (for example A36 to A6) |
|---|---|---|---|
| Thickness | Under 0.230 in | 0.230 to 1.000 in | Typically 3/16 in and up |
| Form | Coil or cut lengths | Coil, used directly or cut into blanks | Discrete plate, or plate cut from coil and tested as plate |
| Tolerances | ASTM A568 or A749 | ASTM A635 | ASTM A6 |
| Typical use | Light brackets, frames, panels | Blanking, forming, tube mill feed | Structural and fabricated plate parts |
Under A1018, coil can be fed directly into a blanking, forming or drawing line, a tube mill or a rolling mill, or it can be sheared or slit into blanks that are formed later. What it cannot become, on paper, is structural plate or pressure vessel plate unless it is tested under ASTM A6 (for plate produced from coil) or ASTM A20 (for pressure vessel plate). Once converted and tested that way, the plate specification governs the converted plate.
In practice this matters most for structural work. If a project specification calls for A36 or A572 plate with A6 tolerances and testing, material leveled and cut from heavy coil has to be certified as plate to that standard, not simply shipped as A1018. For brackets, gussets, base plates and formed parts that are not governed by a plate specification, A1018 material is often the more economical source.
Tip: Material leveled and cut from heavy coil can carry residual stress. Heavily cut parts, such as long narrow strips or plates with large cutouts, may move slightly after laser or plasma cutting. Flag flatness-critical parts on the RFQ.
Testing and certification
For designations with mandatory strength, the mill reports both the heat analysis and tension test results, and the material must meet the minimums for the grade ordered. For CS and DS, the heat analysis is the main certified value. When coil is converted into plate, ASTM A6 or A20 adds its own testing for plate produced from coil, which is why converted plate carries its own test results.
Ask for mill test reports at the time of order when parts feed regulated or defense work, and keep the heat number traceable from coil to finished part. That traceability is what lets a fabricator tie a blank back to its certified chemistry and strength.
What to write on a purchase order
- ASTM A1018 (or A1018M) and year of issue
- Hot rolled heavy-thickness coil, sheet or strip
- Designation with type, grade or class (for example SS Grade 36 Type 2 or HSLAS Grade 50 Class 1)
- Finish (as rolled or pickled), oiled or dry, and edge condition
- Thickness, width, and coil size or cut length
- Whether the material must be converted to plate and certified to ASTM A6 or A20
- Certification required, quantity and part number
Example: ASTM A1018-XX, hot rolled heavy-thickness sheet, SS Grade 36 Type 2, pickled and oiled, 0.250 x 60 in x coil, mill test report required, for formed equipment brackets. For lighter hot rolled gauges, use ASTM A1011 instead.
A1018 material from ASA
ASTM A1018 is on American Steel & Aluminum’s stock list for hot rolled carbon steel. ASA cuts heavier material on CNC plasma and oxy-fuel plate cutting tables up to 10 x 24 ft, forms it on press brakes up to 385 tons and supplies mill certifications with full traceability. Use the steel plate weight calculator to estimate part weights before you request a quote.
Frequently asked questions
What is the difference between ASTM A1011 and A1018?
Both cover hot rolled carbon and high-strength steel in coil form. A1011 covers sheet and strip up to just under 0.230 in thick. A1018 covers heavy-thickness coils from 0.230 in through 1.000 in, with dimensional tolerances from ASTM A635. The designations are similar, so the deciding factor is thickness: order the specification that matches it.
Can A1018 steel be used in place of A36 plate?
Only with care. A1018 SS Grade 36 Type 2 has strength comparable to A36, but A1018 material cannot be sold as structural plate unless it is tested to ASTM A6 rules for plate produced from coil. If a project specification requires A36 plate, ask for plate certified to A36 and A6, not A1018 material.
What thickness range does ASTM A1018 cover?
A1018 covers hot rolled coil from 0.230 in through 1.000 in (6.0 to 25 mm) thick. Strip is material over 8 to 12 in wide, and sheet is over 12 in wide. Thinner hot rolled coil falls under ASTM A1011, and material thicker than 1 in is produced as discrete plate rather than coil.
What tolerances apply to A1018 material?
Thickness, width, camber and flatness tolerances for A1018 coil come from ASTM A635, the general requirements specification for heavy-thickness hot rolled coils. Plate produced from that coil and certified to a plate specification follows the ASTM A6 tolerances instead. Name the tolerance basis on the order when parts are dimensionally critical.