ASTM A1008: Cold Rolled Steel Sheet Specification Explained

How ASTM A1008 classifies cold rolled steel sheet, which designations carry guaranteed strength, and how to write a complete purchase order.

Updated October 2026 7 min read By the ASA team

On this page
  1. What ASTM A1008 covers
  2. A1008 designations explained
  3. Structural and high-strength grades
  4. Exposed, unexposed, finish and aging
  5. A1008 compared with A1011
  6. What to write on a purchase order
  7. Buying A1008 sheet from ASA

ASTM A1008 is the standard specification for cold rolled carbon steel sheet in coils and cut lengths. It sorts the sheet into designations by how it will be used: commercial and drawing steels (CS, DS, DDS, EDDS) that are bought for formability, and structural and high-strength grades (SS, HSLAS, HSLAS-F, SHS, BHS) that are bought to a guaranteed minimum strength.

That split is the most useful thing to understand about the spec. For forming designations, A1008 controls chemistry and gives only typical strength values; for structural and HSLAS designations, minimum yield and tensile strength are mandatory and tested. The values below are from ASTM A1008/A1008M-18; always check the edition named on your order.

What ASTM A1008 covers

A1008 covers cold rolled sheet made from carbon steel, structural steel, high-strength low-alloy steel, solution hardened steel and bake hardenable steel. It was first approved in 2000 and is maintained by ASTM Subcommittee A01.19 on steel sheet and strip. Cold rolled strip is a separate product under ASTM A109 and is not covered.

A1008 is a product specification that leans on a general requirements document. ASTM A568 supplies the thickness, width, length and flatness tolerances, the definitions of surface condition, retest rules and much of the testing detail. When a buyer asks for a tighter tolerance than A1008 sheet normally carries, the starting point is the tables in A568.

The spec also sets defaults that apply when an order is silent. Sheet is furnished with a matte finish and oiled unless the order says otherwise. If no type is given for CS or DS, Type B is supplied. If no class is given for HSLAS, Class 1 is supplied, and SS Grades 33 and 40 default to Type 1.

A1008 designations explained

DesignationWhat it isStrength valuesTypical use
CS Types A, B, CCommercial SteelTypical only (nonmandatory)General bending, brackets, panels, moderate forming
DS Types A, BDrawing SteelTypical onlyDrawn and formed parts with more stretch
DDSDeep Drawing SteelTypical onlyDeep draws, severe forming
EDDSExtra Deep Drawing Steel (stabilized, nonaging)Typical onlyThe most severe draws
SFSSpecial Forming Steel, ordered with a chemistry grade such as 1010Agreed on the orderHigher carbon chemistries that still need formability
SS Grades 25 to 80Structural SteelMandatory minimumsLoad-bearing parts designed to a yield strength
HSLAS Classes 1 and 2High-Strength Low-Alloy SteelMandatory minimumsHigher strength at lower weight
HSLAS-FHSLAS with Improved FormabilityMandatory minimumsHigh strength parts with tighter bends
SHS, BHSSolution Hardened and Bake Hardenable SteelMandatory minimumsPainted panels where paint baking adds strength (BHS)

Commercial Steel is the everyday designation for brackets, covers, panels and general fabrication. CS Type B, with carbon held between 0.02 and 0.15%, is the most widely used because it avoids the ultra-low carbon steels that Type A and Type C allow. Drawing Steel, DDS and EDDS step up in drawability, with lower carbon and aluminum killed or stabilized steelmaking.

A1008 lets buyers combine a designation with a standard chemistry grade from ASTM A568, so an order can call for CS Type B-1008 or DS Type A-1005. That is how sheet specified as C1008 or C1010 on a drawing is usually bought: see the guide to 1006, 1008 and 1010 low carbon steel for how those chemistries differ.

Chemistry of the forming designations

DesignationCarbon (%)Manganese, max (%)Note
CS Type A0.10 max0.60Can be supplied below 0.02% carbon
CS Type B0.02 to 0.150.60Furnished when no type is specified
CS Type C0.08 max0.60Phosphorus up to 0.10%
DS Type A0.08 max0.50Aluminum killed (0.01% Al min)
DS Type B0.02 to 0.080.50Aluminum killed (0.02% Al min)
DDS0.06 max0.50Aluminum killed
EDDS0.02 max0.40Vacuum degassed and stabilized

For CS, DS, DDS and EDDS, the heat analysis is what the mill guarantees. The standard also caps phosphorus, sulfur and residual elements.

Typical properties are not guarantees

DesignationTypical yield strengthTypical elongation in 2 in
CS Types A, B, C20 to 40 ksi (140 to 275 MPa)30% or more
DS Types A, B22 to 35 ksi (150 to 240 MPa)36% or more
DDS17 to 29 ksi (115 to 200 MPa)38% or more
EDDS15 to 25 ksi (105 to 170 MPa)40% or more

These ranges are nonmandatory. They describe what the designation usually delivers so a buyer can pick the right one, and the standard notes that values outside them are to be expected. Yield strength tends to rise, and elongation to fall, as sheet gets thinner. If a design calculation depends on a strength value, order an SS or HSLAS designation instead of CS.

Structural and high-strength grades

In the SS, HSLAS and HSLAS-F designations, the grade number is the minimum yield strength in ksi. These minimums are mandatory, and the mill must report heat analysis and tension test results. The table shows the structural grades and a sample of the high-strength grades.

DesignationYield, minTensile, minElongation in 2 in, min
SS Grade 2525 ksi (170 MPa)42 ksi (290 MPa)26%
SS Grade 3030 ksi (205 MPa)45 ksi (310 MPa)24%
SS Grade 33, Types 1 and 233 ksi (230 MPa)48 ksi (330 MPa)22%
SS Grade 40, Types 1 and 240 ksi (275 MPa)52 ksi (360 MPa)20%
SS Grade 4545 ksi (310 MPa)60 ksi (410 MPa)20%
SS Grade 5050 ksi (340 MPa)65 ksi (450 MPa)18%
SS Grade 6060 ksi (410 MPa)75 ksi (520 MPa)12%
SS Grade 7070 ksi (480 MPa)85 ksi (585 MPa)6%
SS Grade 8080 ksi (550 MPa)82 ksi (565 MPa)No requirement
HSLAS Grade 50, Class 150 ksi (340 MPa)65 ksi (450 MPa)20%
HSLAS Grade 50, Class 250 ksi (340 MPa)60 ksi (410 MPa)20%
HSLAS-F Grade 5050 ksi (340 MPa)60 ksi (410 MPa)22%

HSLAS grades come in two classes. Class 2 has a lower carbon ceiling (0.15% max) and a minimum tensile strength 5 ksi below Class 1 at the same yield, which gives slightly better formability and weldability. HSLAS-F goes further: it is fully killed, fine grain, treated for inclusion control, and microalloyed with elements such as columbium (niobium) and vanadium.

The nonmandatory bend guidance in the standard shows the difference in practice. Suggested minimum inside radii for a 90 degree cold bend are 1-1/2 t for SS Grade 33, 2 t for SS Grade 40 and 2-1/2 t for SS Grade 50, while HSLAS-F Grade 50 is listed at 1 t. SS Grade 80 is a full hard product with no elongation requirement and is not intended for cold bending.

The mill runs two tension tests per heat or per 50 tons. Coils are tested at the end, but the whole coil must meet the minimums.

Exposed, unexposed, finish and aging

Every A1008 order is classified as exposed or unexposed. Exposed sheet is for visible, painted surfaces where appearance matters, such as appliance panels and enclosure doors. Unexposed sheet is for hidden or noncritical parts and is specified as either temper rolled or annealed last, with the details of each in ASTM A568.

Aging is the other surface issue. CS, DS and DDS sheet can age: it loses ductility and gains hardness over time after temper rolling, which makes stretcher strains and fluting more likely when the sheet is formed later. EDDS is stabilized and nonaging. For other designations, the standard advises consulting the supplier, and the practical answer is to form aging-sensitive sheet reasonably soon after it is processed.

Tip: For visible painted parts, put “exposed” on the order. Unexposed sheet can carry surface marks that are acceptable for hidden parts but show through paint and powder coat.

A1008 compared with A1011

PointASTM A1008 (cold rolled)ASTM A1011 (hot rolled)
Default surfaceMatte finishAs rolled, with mill scale; pickled or blast cleaned on request
Default oilingOiledDry as rolled; oiled when pickled
Forming designationsCS, DS, DDS, EDDS, SFSCS (Types A to D), DS
Strength designationsSS, HSLAS, HSLAS-F, SHS, BHSSS, HSLAS, HSLAS-F, UHSS
General requirementsASTM A568ASTM A568 (sheet), ASTM A749 (strip)

Cold rolled A1008 sheet comes in thinner gauges, with a smoother surface and tighter thickness tolerances than hot rolled sheet, which is why it is the usual choice for precision sheet metal, enclosures and painted parts. Hot rolled sheet under ASTM A1011 usually costs less per pound and suits heavier gauges and parts where surface finish is secondary.

What to write on a purchase order

A1008 puts the responsibility for a complete description on the purchaser. A useful order includes:

  • ASTM A1008 (or A1008M for metric) and the year of issue
  • Product name and designation, with type, grade or class as applicable
  • Exposed or unexposed; temper rolled or annealed last for unexposed sheet
  • Finish, and oiled or not oiled
  • Thickness as a decimal, width, and length or coil, with coil ID, OD and maximum weight
  • Copper bearing steel, if required
  • Quantity, part number or application, and certification requirements

Two example callouts (replace XX with the edition year your order requires):

  • ASTM A1008-XX, cold rolled steel sheet, CS Type B, unexposed, matte finish, oiled, 0.0598 x 48 x 120 in, 200 sheets, for enclosure side panel.
  • ASTM A1008-XX, cold rolled steel sheet, SS Grade 40 Type 1, exposed, matte finish, oiled, 0.0747 x 60 x 120 in, mill test report with heat analysis and tensile results.

Write the decimal thickness rather than relying on a gauge number. The sheet metal gauge chart converts gauges to decimals if your drawing uses them.

Buying A1008 sheet from ASA

ASTM A1008 is on American Steel & Aluminum’s stock list for cold rolled sheet, alongside C1006, C1008, C1010 and HSLA chemistries. ASA can level and cut carbon sheet from 24 to 11 gauge on its leveling and cut-to-length line, then laser cut, form and weld parts in-house, with mill certifications and full traceability. Request a quote with the designation, thickness and quantity you need.

Frequently asked questions

Is ASTM A1008 the same as 1008 steel?

No. ASTM A1008 is a product specification for cold rolled sheet, while 1008 is a chemistry grade with defined carbon and manganese ranges. The two are often combined: an order for A1008 CS Type B with chemistry grade 1008 gets sheet made to the 1008 chemistry and supplied under the A1008 rules for tolerances, finish, oiling and certification.

Does ASTM A1008 commercial steel have a minimum yield strength?

No. For CS, DS, DDS and EDDS, the standard lists only typical, nonmandatory mechanical properties. Commercial Steel typically yields between 20 and 40 ksi, but values outside that range are allowed. If a part is designed to a strength value, order a structural (SS) or high-strength low-alloy (HSLAS) designation, which carries tested minimums.

What is the difference between HSLAS Class 1 and Class 2?

Both classes have the same minimum yield strength for a given grade. Class 2 is limited to 0.15% carbon and has a minimum tensile strength 5 ksi lower than Class 1, which generally improves formability and weldability. If the order does not name a class, the mill supplies Class 1, so specify Class 2 when tighter bends matter.

What does exposed mean on a cold rolled steel order?

Exposed sheet is intended for surfaces that will be seen, usually after painting or powder coating, so it is held to a higher standard of surface quality. Unexposed sheet is for hidden or noncritical parts and may show marks that would read through a finish. The choice changes how the sheet is processed and inspected, so it belongs on every A1008 order.

Can ASTM A1008 sheet be welded?

Yes. The standard states that its sheet grades are suitable for welding when appropriate welding conditions are selected. Resistance spot welding, MIG and TIG are all common on cold rolled sheet. If a particular welding process needs tighter chemistry limits, the standard requires them to be specified at inquiry and confirmed when the order is placed.

Material, processing and fabrication from one supplier

Send a drawing or a material list and the ASA team will quote it from stock.