On this page
A36 steel is a low carbon structural steel made to ASTM A36, with a minimum yield strength of 36 ksi (250 MPa) and a tensile strength of 58 to 80 ksi (400 to 550 MPa). It is the default grade for general purpose plate, bar and many structural shapes because it is easy to weld, cut, form and machine at a low cost per pound.
The specification covers carbon steel plates, shapes and bars for bolted, riveted or welded construction in bridges, buildings and general structural work. Below are the chemistry limits by product form, the mechanical properties, how A36 behaves in the shop, and where it fits next to A992 and other grades.
A36 chemical composition
ASTM A36 controls chemistry with maximum limits rather than a tight target range, and the limits change with product form and thickness. Carbon is capped at 0.25 to 0.29% depending on the product, sulfur at 0.05% and phosphorus at 0.04% in the long-standing A36 tables (some current mill data sheets show a tighter 0.030% phosphorus limit for plate and bar, so check the edition your order cites). When copper bearing steel is specified, copper must be at least 0.20%.
Plate
| Plate thickness | Carbon, max | Manganese | Silicon |
|---|---|---|---|
| To 3/4 in (20 mm) | 0.25% | No requirement | 0.40% max |
| Over 3/4 to 1-1/2 in (20 to 40 mm) | 0.25% | 0.80 to 1.20% | 0.40% max |
| Over 1-1/2 to 2-1/2 in (40 to 65 mm) | 0.26% | 0.85 to 1.20% | 0.15 to 0.40% |
| Over 2-1/2 to 4 in (65 to 100 mm) | 0.27% | 0.85 to 1.20% | 0.15 to 0.40% |
| Over 4 in (100 mm) | 0.29% | 0.85 to 1.20% | 0.15 to 0.40% |
Shapes and bars
| Product | Carbon, max | Manganese |
|---|---|---|
| Structural shapes (most sizes) | 0.26% | No requirement |
| Bars to 3/4 in (20 mm) | 0.26% | No requirement |
| Bars over 3/4 to 1-1/2 in (20 to 40 mm) | 0.27% | 0.60 to 0.90% |
| Bars over 1-1/2 to 4 in (40 to 100 mm) | 0.28% | 0.60 to 0.90% |
| Bars over 4 in (100 mm) | 0.29% | 0.60 to 0.90% |
Silicon is limited to 0.40% max for shapes and bars, and the phosphorus and sulfur limits above apply across these forms. Shapes with flanges over 3 in (75 mm) thick also require 0.85 to 1.35% manganese and 0.15 to 0.40% silicon. The rising manganese requirements in thicker plate and bar, and the silicon range in heavy plate, help the steel reach 36 ksi through the full section, since heavy sections cool more slowly at the mill and would otherwise come out weaker.
A36 mechanical properties
The mechanical requirements are what most buyers and engineers care about. A36 guarantees a yield floor and a tensile window, plus a minimum elongation that confirms the steel will stretch and bend before it breaks.
| Property | ASTM A36 value |
|---|---|
| Yield strength | 36 ksi (250 MPa) minimum |
| Yield strength, plate over 8 in (200 mm) | 32 ksi (220 MPa) minimum |
| Tensile strength | 58 to 80 ksi (400 to 550 MPa) |
| Elongation in 8 in (200 mm), plates, bars and shapes | 20% minimum |
| Elongation in 2 in (50 mm), plate and bar | 23% minimum |
| Elongation in 2 in (50 mm), shapes | 21% minimum |
| Modulus of elasticity | 29,000 ksi (200 GPa), typical |
| Density | 0.284 lb/in³ (7.85 g/cm³), typical |
Because 36 ksi is a minimum, actual mill test values are often higher. Designers should still use the specified minimum in calculations. If a project needs a guaranteed higher yield, specify a higher strength grade rather than counting on overstrength in A36.
Weldability, machinability and formability
Welding
A36 is one of the easiest structural steels to weld. Its low carbon content and modest alloy levels keep hardenability low, so the heat affected zone is unlikely to form brittle martensite in normal section sizes. It welds well with common processes (MIG, flux core, stick and submerged arc) using standard E70 series filler metals.
Thick sections need more care. As plate gets heavier, the steel pulls heat away from the weld faster, so preheat is often required to prevent hydrogen cracking. Structural welding codes such as AWS D1.1 list A36 as a prequalified base metal and set minimum preheat by thickness.
Tip: Mill scale on hot rolled A36 can cause porosity and poor fusion. Grind or blast weld zones on critical joints, and consider pickled and oiled sheet for thin parts that will be painted or powder coated.
Machining and cutting
A36 machines reasonably well, though it is softer and gummier than free machining grades, so chip control is the main issue on long runs. It cuts cleanly on fiber laser, plasma and oxy-fuel equipment. Oxy-fuel is the usual choice for very heavy plate, while laser gives the tightest edges on thinner gauges.
Forming
The required elongation means A36 bends well on a press brake. Bend radius depends on thickness and grain direction: a bend line running perpendicular to the rolling direction allows a tighter radius than one running parallel to it. Heavier plate needs a larger inside radius as a multiple of its thickness, so check the minimum radius for the gauge or plate size before finalizing a drawing.
Common uses of A36 steel
A36 shows up wherever moderate strength, low cost and easy fabrication matter more than weight savings or corrosion resistance. Typical applications include:
- Base plates, connection plates, gussets and clip angles in building and structural work
- Frames, skids, brackets and weldments for industrial equipment
- Machine bases and fixtures that are later machined or Blanchard ground
- Platforms, stairs, ladders and mezzanine components
- Tanks, bins and hoppers where corrosion is handled with paint or coating
- Racking, enclosures and support structures for data center and energy storage projects
A36 has no meaningful corrosion resistance on its own. Outdoors or in wet service it needs paint, powder coat or galvanizing. Where the environment is too aggressive for a coating, compare carbon steel vs stainless steel on lifetime cost rather than material price alone.
A36 vs A992 and other grades
A36 is no longer the dominant grade for wide flange beams. Most W shapes are now produced to ASTM A992, which has a 50 ksi (345 MPa) minimum yield, a 65 ksi (450 MPa) minimum tensile, a maximum yield to tensile ratio and tighter chemistry controls suited to seismic design. Plate, angle, channel and bar, however, are still very commonly specified as A36.
| Grade | Min yield | Typical products |
|---|---|---|
| ASTM A36 | 36 ksi (250 MPa) | Plate, bar, angle, channel |
| ASTM A992 | 50 ksi (345 MPa) | Wide flange beams |
| ASTM A572 Grade 50 | 50 ksi (345 MPa) | Plate and shapes needing higher strength |
| ASTM A588 | 50 ksi (345 MPa) | Weathering steel for exposed structures |
Many shapes are dual certified so a single mill heat meets more than one specification. Check the mill test report for the grades listed before substituting. For thin flat-rolled sheet, the comparable products are usually ordered to ASTM A1011 (hot rolled) or ASTM A1008 (cold rolled) rather than A36.
A36 on ASA’s stock list
A36 appears on ASA’s carbon steel stock list in two product lines:
- Plate and flat-rolled: hot rolled A36 alongside other carbon grades such as C1008, C1010, C1045 and HSLA, in the flat-rolled sheet and plate line
- Structural shapes: angle, channel and wide flange beam, with A36, A992, A709 and A588 on the stock list
ASA also stocks carbon steel bar (flats, squares and rounds) and structural and mechanical steel tube. Structural tube is normally produced to its own specifications, such as ASTM A500, rather than A36, so name the grade and specification you need for bar and tube when you ask for a quote. To estimate plate weight before quoting, use the steel plate weight calculator.
Buying and processing A36 with ASA
American Steel & Aluminum supplies A36 flat-rolled steel and structural shapes from five Northeast locations, with mill certifications and full material traceability available. ASA can also cut it to your print on CNC plasma and oxy-fuel plate cutting tables that handle carbon steel up to 8 in thick, then form, weld and powder coat the parts in house. A company-owned truck fleet serves New England and New York, and JIT delivery gets most orders to customers in 24 to 48 hours. Start with a request for a quote.
Frequently asked questions
Is A36 steel the same as mild steel?
Mild steel is an informal name for low carbon steel, usually below about 0.25 to 0.30% carbon. A36 is a specific ASTM standard that falls inside that family but also guarantees mechanical properties: at least 36 ksi yield and 58 to 80 ksi tensile. Ordering "mild steel" gives no guaranteed strength, so engineers specify A36 or another named grade on drawings.
Can A36 steel be heat treated?
A36 responds poorly to through hardening because its carbon content is low. It can be normalized or stress relieved, and the surface can be case hardened by carburizing if a wear face is needed. Parts that need high hardness through the section are usually made from medium carbon grades such as C1045 instead.
Does A36 steel rust?
Yes. A36 is plain carbon steel with no chromium, so it rusts when exposed to moisture and oxygen. Indoors, a light oil film or primer may be enough. Outdoors, it needs a protective system such as paint, powder coating or hot-dip galvanizing. For exposed structures without coating, a weathering grade like A588 is the more common choice.
What is the difference between A36 and A572 Grade 50?
Both are carbon structural steels, but A572 Grade 50 is a high strength low alloy grade with a 50 ksi minimum yield versus 36 ksi for A36. That higher strength can allow lighter sections. A572 reaches that strength with small additions of elements such as niobium or vanadium, while keeping good weldability.
Is A36 steel magnetic?
Yes. Like other carbon steels, A36 has a ferritic and pearlitic structure and is strongly magnetic. That makes it easy to hold with magnetic lifters and fixtures in the shop. It also means a magnet will not help tell A36 apart from other carbon grades; a mill test report or chemical analysis is needed for that.