316L Stainless Steel: Properties and Uses in Welded Parts

Why 316L stainless steel, the low-carbon version of 316, is the default for welded parts in marine, chemical and pharmaceutical service, with ASTM A240 properties and welding guidance.

Updated October 2026 5 min read By the ASA team

On this page
  1. 316L composition compared with 316
  2. Mechanical and physical properties
  3. Why 316L is the default for welded parts
  4. Welding and finishing 316L parts
  5. Common uses of 316L stainless steel
  6. Buying 316L stainless from ASA

316L stainless steel is the low-carbon version of 316, with carbon limited to 0.030% maximum while keeping the same 2 to 3% molybdenum. It offers the chloride resistance of 316 without the risk of sensitization in heat-affected zones, which makes it the default choice for welded parts in marine, chemical, pharmaceutical and food processing service.

Under ASTM A240, annealed 316L must meet at least 70 ksi (485 MPa) tensile and 25 ksi (170 MPa) yield strength. Dual-certified 316/316L also meets the higher 316 minimums, so many fabricators stock one material for both.

316L composition compared with 316

316L is designated UNS S31603 and is roughly equivalent to EN 1.4404. These are the ASTM A240 limits for flat-rolled sheet, strip and plate (weight percent):

Element316 (S31600)316L (S31603)
Carbon0.08 max0.030 max
Manganese2.00 max2.00 max
Silicon0.75 max0.75 max
Phosphorus0.045 max0.045 max
Sulfur0.030 max0.030 max
Chromium16.0 to 18.016.0 to 18.0
Nickel10.0 to 14.010.0 to 14.0
Molybdenum2.00 to 3.002.00 to 3.00
Nitrogen0.10 max0.10 max

Carbon is the only difference. Chromium, nickel and molybdenum are identical, so in the annealed condition 316L resists pitting and crevice corrosion exactly as 316 does, with a typical PREN of about 23 to 25. The benefit of low carbon shows up only once the metal has been welded or otherwise heated.

Flat-rolled 316L is ordered to ASTM A240, with ASTM A480 covering general requirements such as tolerances and finish, or to ASME SA240 and SA480 for pressure vessel work. Name the grade, the specification and any dual-certification requirement on the purchase order, since 316L cannot be told apart from 316 or 304 by eye.

Mechanical and physical properties

Mechanical properties (ASTM A240, annealed)

Property316L316
Tensile strength, min70 ksi (485 MPa)75 ksi (515 MPa)
Yield strength (0.2% offset), min25 ksi (170 MPa)30 ksi (205 MPa)
Elongation in 2 in (50 mm), min40%40%
Hardness, max95 HRB (217 HBW)95 HRB (217 HBW)

The 5 ksi lower strength minimums rarely matter in sheet metal parts, enclosures or brackets, but they lower code allowable stresses in pressure equipment. Dual-certified 316/316L closes that gap. Like 316, the grade gains strength from cold work and cannot be hardened by heat treatment.

Physical properties (typical)

PropertyTypical value
Density0.289 lb/in³ (8.00 g/cm³)
Modulus of elasticity28,000 ksi (193 GPa)
Mean thermal expansion, 32 to 212°F (0 to 100°C)8.9 µin/in·°F (16.0 µm/m·°C)
Thermal conductivity at 212°F (100°C)9.4 Btu/hr·ft·°F (16.3 W/m·K)

Physical properties match 316, and 316L is likewise nonmagnetic when annealed. The full set, including resistivity and melting range, is in the 316 stainless steel guide.

Why 316L is the default for welded parts

When the metal beside a weld passes through roughly 800 to 1500°F (425 to 815°C), carbon in the steel can combine with chromium to form carbides at the grain boundaries. That strips chromium from the surrounding metal and leaves paths that corrode preferentially. The condition is called sensitization, and the resulting attack is intergranular corrosion.

Chloride and acid environments are exactly where sensitized metal fails, and they are also where 316 is used. Pairing molybdenum with low carbon means the welds and heat-affected zones keep the same corrosion resistance as the plate, without solution annealing the finished assembly. For a fuller explanation of the mechanism and testing, see the guide to 304L stainless steel; the chemistry works the same way.

Low carbon also helps with other heat exposures that hold metal in the sensitizing range far longer than a weld does, such as stress relieving an assembly or hot forming a heavy section.

Standard 316 can still be the right choice for thin sheet with short single-pass welds, for parts that are not welded at all, or for parts that will be annealed after fabrication.

Dual-certified 316/316L

Much of the 316L made today is certified as 316/316L. It meets the 0.030% carbon limit of 316L and the 75 ksi (515 MPa) tensile and 30 ksi (205 MPa) yield minimums of 316, usually through careful use of the nitrogen allowance. The mill test report lists both grades. If a drawing calls for both properties, state it on the purchase order and check the certification.

Welding and finishing 316L parts

316L welds readily by TIG, MIG and stick processes with ER316L filler metal, which matches the molybdenum of the base metal so the weld bead resists chlorides as well as the plate. ER316LSi improves wetting in MIG work. No preheat is required. On full-penetration welds in tube or closed sections, purge the back side with argon so the root does not oxidize.

Welding leaves heat tint, the straw to blue oxide colors beside the bead. That oxide is thicker but less protective than the natural passive film, and in chloride service it is often where pitting starts. Remove it by pickling, mechanical cleaning or electropolishing, then passivate. ASTM A380 covers cleaning, descaling and passivation practice, and ASTM A967 covers chemical passivation treatments.

Tip: On marine and process equipment, put heat tint removal and passivation on the drawing or purchase order. A 316L weldment left with heat tint can stain or pit sooner than a properly cleaned 304 part.

Cutting comes before welding on most 316L parts. Fiber laser cutting with nitrogen assist produces a bright, oxide-free edge that is ready to weld, while thicker plate is often plasma cut and then cleaned back to bright metal at the weld prep. Either way, keep cut edges free of iron contamination from carbon steel work sharing the same equipment.

316L forms on the press brake much like 304, with good ductility, more springback than carbon steel and higher bending loads. ASA’s press brake forming handles stainless from prototype through production.

Common uses of 316L stainless steel

  • Pharmaceutical and biotech process equipment, which is heavily welded and frequently polished or electropolished
  • Food, dairy and beverage equipment exposed to brines or chloride-based sanitizers
  • Marine weldments, boat fittings and shipboard components
  • Chemical tanks, vessels and process skids
  • Coastal enclosures, frames, railings and architectural weldments
  • Water and wastewater treatment equipment

In each case the part is welded and the environment is aggressive enough that a sensitized weld zone would be the first place to fail. Where parts are not welded, or the environment is mild, 316 or even 304 may do the same job for less.

Buying 316L stainless from ASA

ASA stocks 316L stainless along with 316, 304 and 304L, with mill certifications and full material traceability available. Its fiber laser, press brakes, and manual and robotic welding turn 316L into finished weldments under an ISO 9001:2015 certified quality system. Request a quote for 316L parts or material with your specification and any dual-certification requirement.

Frequently asked questions

Is 316L better than 316?

316L is better for welded parts, because its 0.030% carbon limit prevents sensitization in heat-affected zones. 316 has slightly higher guaranteed strength. For unwelded parts both resist corrosion equally. Since dual-certified 316/316L combines low carbon with the higher strength minimums, many fabricators simply buy dual-certified stock and use it for both purposes.

Is 316L stainless steel magnetic?

316L is nonmagnetic when annealed. Heavy cold work can introduce a slight magnetic response, and weld metal is normally designed to contain a small amount of ferrite to prevent hot cracking, so welds may attract a magnet weakly. Neither condition indicates a problem with the material or with its corrosion resistance.

What filler metal should be used to weld 316L?

ER316L is the standard filler metal for 316L, available as TIG rod and MIG wire, with ER316LSi offering better wetting in MIG work. It carries molybdenum so the weld resists chlorides as well as the plate does. Joining 316L to carbon steel typically uses ER309L or ER309LMo instead, which tolerate dilution from the carbon steel.

Why is 316L used in pharmaceutical equipment?

Pharmaceutical and biotech equipment is heavily welded, cleaned often with aggressive chemicals, and must not shed corrosion products into the product. 316L combines molybdenum for chloride resistance with low carbon that protects every weld seam. It also responds well to mechanical polishing and electropolishing, producing the smooth, cleanable surfaces those industries require.

Does 316L need to be passivated after welding?

Passivation is recommended whenever the part will see a corrosive environment. Welding, grinding and handling leave heat tint and embedded iron that weaken the protective oxide layer. Removing heat tint by pickling or mechanical cleaning, followed by a chemical passivation treatment to ASTM A967 or A380, restores full corrosion resistance across the weld zone.

Material, processing and fabrication from one supplier

Send a drawing or a material list and the ASA team will quote it from stock.