316 Stainless Steel: Properties, Composition and Uses

The chemistry, ASTM A240 properties and corrosion behavior of 316 stainless steel, and why its molybdenum makes it the go-to grade for marine, coastal and chemical service.

Updated October 2026 5 min read By the ASA team

On this page
  1. Chemical composition of 316 stainless steel
  2. Mechanical and physical properties
  3. How molybdenum improves corrosion resistance
  4. Marine, chemical and other uses of 316
  5. Welding and fabricating 316
  6. 316 vs 304 and 316L
  7. Buying 316 stainless from ASA

316 stainless steel is an austenitic stainless steel with 16 to 18% chromium, 10 to 14% nickel and 2 to 3% molybdenum. The molybdenum gives it markedly better resistance to pitting and crevice corrosion from chlorides than 304, which makes 316 the standard grade for marine, coastal, chemical processing and pharmaceutical equipment.

Under ASTM A240, annealed 316 has the same minimum strength as 304: 75 ksi (515 MPa) tensile and 30 ksi (205 MPa) yield. It forms and welds much like 304 but costs more, so the choice between them usually comes down to the environment the part will see.

Chemical composition of 316 stainless steel

316 is designated UNS S31600 and is roughly equivalent to EN 1.4401. The table shows the chemistry limits ASTM A240 sets for flat-rolled 316 sheet, strip and plate.

ElementASTM A240 limit (wt%)
Carbon0.08 max
Manganese2.00 max
Silicon0.75 max
Phosphorus0.045 max
Sulfur0.030 max
Chromium16.0 to 18.0
Nickel10.0 to 14.0
Molybdenum2.00 to 3.00
Nitrogen0.10 max
IronBalance

Compared with 304, 316 trades a little chromium for molybdenum and carries more nickel. Molybdenum tends to promote ferrite, so the higher nickel range keeps the structure fully austenitic, tough and nonmagnetic in the annealed condition. The 0.08% carbon limit is slightly higher than 304’s 0.07%, which is why heavy welded work usually calls for the low-carbon version, 316L.

Order flat-rolled 316 to ASTM A240, with ASTM A480 covering general requirements such as tolerances, flatness and finish, or to ASME SA240 and SA480 for code work. Because 316 and 304 look identical, the specification and the mill certification are the only practical proof of what you received. Handheld XRF or a molybdenum spot test can confirm the grade at receiving when parts are critical.

Mechanical and physical properties

Mechanical properties (annealed)

PropertyASTM A240 requirement
Tensile strength75 ksi (515 MPa) min
Yield strength (0.2% offset)30 ksi (205 MPa) min
Elongation in 2 in (50 mm)40% min
Hardness95 HRB (217 HBW) max

These are specification minimums plus a hardness maximum; mill test results normally exceed them, and the certification for each heat reports the measured values. Like all austenitic grades, 316 cannot be hardened by heat treatment but gains considerable strength from cold work. It also holds its strength at elevated temperature somewhat better than 304, which is one reason it appears in heat exchangers and high-temperature process equipment.

Physical properties (typical)

PropertyTypical value
Density0.289 lb/in³ (8.00 g/cm³)
Modulus of elasticity28,000 ksi (193 GPa)
Mean thermal expansion, 32 to 212°F (0 to 100°C)8.9 µin/in·°F (16.0 µm/m·°C)
Thermal conductivity at 212°F (100°C)9.4 Btu/hr·ft·°F (16.3 W/m·K)
Electrical resistivity74 µΩ·cm
Melting range2500 to 2550°F (1370 to 1400°C)

As with 304, high thermal expansion and low thermal conductivity concentrate heat and increase distortion during welding and cutting compared with carbon steel. Annealed 316 is nonmagnetic, and its higher nickel content means it usually picks up less magnetism than 304 after bending or cold rolling.

How molybdenum improves corrosion resistance

Chlorides attack stainless steel locally rather than evenly. They break down the passive film at weak points such as inclusions, scratches or crevices, and the small anodic site that results can grow into a deep pit while the rest of the surface looks fine. Molybdenum strengthens the passive film and helps it repair itself in chloride-bearing conditions, so pits are harder to start and slower to grow.

The usual way to compare grades is the pitting resistance equivalent number: PREN = %Cr + 3.3 x %Mo + 16 x %N. Typical 316 scores about 23 to 25, against about 18 to 20 for 304. A common rule of thumb in water service puts the chloride limit for 316 at roughly 1,000 ppm at ambient temperature, compared with roughly 200 ppm for 304. Molybdenum also improves resistance to sulfuric, phosphoric and acetic acids and to many reducing chemicals.

Limits of 316

  • Seawater immersion: stagnant or warm seawater, fouling and tight crevices under gaskets can still cause crevice corrosion. Permanently submerged parts often need a higher-alloy stainless steel.
  • Stress corrosion cracking: above about 140°F (60°C), chlorides combined with tensile stress can crack 316, as they can 304.
  • Welded heavy sections: the heat-affected zone can become sensitized; 316L avoids this.

Marine, chemical and other uses of 316

  • Boat hardware, deck fittings, railings and other marine-grade components
  • Coastal architectural panels, handrails and outdoor enclosures exposed to salt air
  • Chemical processing tanks, vessels and equipment handling chlorides or sulfuric and phosphoric acids
  • Pharmaceutical and medical equipment where cleanliness and corrosion resistance matter
  • Food processing that involves brines, salt or chloride-based sanitizers
  • Water and wastewater treatment equipment
  • Street furniture, vehicle parts and equipment exposed to deicing salts

The common thread is chloride exposure. In clean, dry or freshwater service, 316 gives little practical advantage over 304, so the extra cost buys nothing.

Welding and fabricating 316

316 welds well by TIG, MIG and stick processes with no preheat. ER316L is the most common filler metal because it matches the molybdenum of the base metal while keeping weld metal carbon low; ER316LSi is popular for MIG work. For heavy sections and multi-pass welds that will not be annealed after welding, specify 316L stainless steel to avoid sensitization in the heat-affected zone.

On the press brake, 316 behaves much like 304, with high ductility, more springback than carbon steel and higher forming loads. Its more stable austenite work hardens at a slightly lower rate than 304, but machining still calls for sharp tools, steady feeds and enough depth of cut to stay under the hardened layer. Fiber laser cutting with nitrogen assist leaves a clean, oxide-free edge, which matters on parts that must keep full corrosion resistance at the cut edge.

Tip: Paying for 316 does not protect a part from iron contamination. Use stainless-only brushes and abrasives, and passivate finished parts that will see marine or chemical exposure, or embedded iron will stain the surface.

316 vs 304 and 316L

GradeKey differenceChoose it when
304No molybdenum, lower nickel, lower costIndoor, freshwater and mild outdoor service
3162 to 3% molybdenum, 0.08% carbon maxChloride exposure, thin welded or unwelded parts
316LSame molybdenum, 0.030% carbon maxHeavy welded parts in chloride or chemical service

For a detailed side-by-side on cost, PREN, magnetism and application, see 304 vs 316 stainless steel. For the base grade, see the guide to 304 stainless steel.

Buying 316 stainless from ASA

ASA stocks 316 and 316L stainless along with 304 and 304L in its sheet and plate line, with mill certifications, full material traceability, and RoHS and DFARS documentation available. ASA also supplies marine-grade and mil-spec materials for defense and shipbuilding programs, and its fiber and tube lasers, press brakes and robotic weld cells turn 316 into finished parts. Request a quote for 316 stainless from any of ASA’s five Northeast locations.

Frequently asked questions

Is 316 stainless steel marine grade?

316 is commonly called marine grade because its molybdenum content resists salt spray and splash far better than 304. It performs well on deck hardware, railings and coastal structures. For permanent immersion in warm or stagnant seawater, crevice corrosion can still occur, and designers often step up to higher-alloy stainless steels for those conditions.

Is 316 stainless steel magnetic?

In the annealed condition 316 is nonmagnetic. Its higher nickel content keeps the austenitic structure more stable than in 304, so it usually picks up less magnetism after bending or cold rolling. Slight attraction near welds or heavily formed areas is normal and is not a sign that the wrong grade was supplied.

Does 316 stainless steel rust?

316 resists rust in far more environments than 304, including coastal air and many chloride-bearing chemicals. It is not immune: crevices, deposits, embedded iron from carbon steel tools, and warm concentrated chlorides can still cause staining or pitting. Regular cleaning, good drainage and proper passivation after fabrication keep 316 surfaces clean and bright.

What is the difference between 316 and 316L?

316L limits carbon to 0.030% compared with 0.08% for 316, which keeps welded areas free of chromium carbides and the intergranular corrosion they cause. 316L has slightly lower minimum strength under ASTM A240. For welded heavy sections 316L is the usual choice, and dual-certified 316/316L material meets both specifications at once.

Can 316 stainless be used for food equipment?

Yes. 316 is widely used in food and beverage processing, particularly where products contain salt, brines or acids, or where chloride-based sanitizers are used for cleaning. It offers the same cleanability as 304 with better resistance to pitting, which helps surfaces stay smooth and sanitary through years of washdowns.

Material, processing and fabrication from one supplier

Send a drawing or a material list and the ASA team will quote it from stock.