On this page
304L stainless steel is the low-carbon version of 304, with carbon limited to 0.030% maximum instead of 0.07%. That lower carbon keeps welds and heat-affected zones resistant to intergranular corrosion, so 304L is the standard choice for heavy welded sections and weldments that will not be annealed after welding.
Otherwise 304L behaves almost exactly like 304: the same 18% chromium and 8% nickel base, the same corrosion resistance in most environments, and effectively the same physical properties. The trade-off is a slightly lower minimum strength, which dual-certified 304/304L material removes.
304L composition compared with 304
304L is designated UNS S30403 and is roughly equivalent to EN 1.4307. ASTM A240 sets these limits for flat-rolled sheet, strip and plate (weight percent):
| Element | 304 (S30400) | 304L (S30403) |
|---|---|---|
| Carbon | 0.07 max | 0.030 max |
| Manganese | 2.00 max | 2.00 max |
| Silicon | 0.75 max | 0.75 max |
| Phosphorus | 0.045 max | 0.045 max |
| Sulfur | 0.030 max | 0.030 max |
| Chromium | 17.5 to 19.5 | 17.5 to 19.5 |
| Nickel | 8.0 to 10.5 | 8.0 to 12.0 |
| Nitrogen | 0.10 max | 0.10 max |
The meaningful differences are the carbon ceiling and a wider nickel range. Carbon is a strong austenite former, so mills can use the extra nickel allowance to keep the structure balanced when carbon is held low. Everything that gives 304 its corrosion resistance, chiefly the chromium, is unchanged.
Mechanical and physical properties of 304L
Annealed minimums under ASTM A240, with 304 shown for comparison:
| Property | 304L | 304 |
|---|---|---|
| Tensile strength, min | 70 ksi (485 MPa) | 75 ksi (515 MPa) |
| Yield strength (0.2% offset), min | 25 ksi (170 MPa) | 30 ksi (205 MPa) |
| Elongation in 2 in (50 mm), min | 40% | 40% |
| Hardness, max | 92 HRB (201 HBW) | 92 HRB (201 HBW) |
Carbon strengthens austenitic stainless steel, so removing most of it lowers the guaranteed tensile and yield strength by 5 ksi (about 30 to 35 MPa). For most sheet metal parts, brackets and enclosures the difference does not matter. In pressure equipment and structural design it can, because code allowable stresses for 304L are lower than for 304.
Density, elastic modulus, thermal expansion and thermal conductivity are effectively the same as 304, and 304L is likewise nonmagnetic when annealed. See the 304 stainless steel guide for typical physical property values.
Sensitization: why low carbon matters
Austenitic stainless steels held in roughly the 800 to 1500°F (425 to 815°C) range can form chromium carbides along their grain boundaries. Each carbide pulls chromium out of the metal around it, leaving narrow chromium-depleted bands that can no longer maintain a passive film. In a corrosive environment those bands are attacked first, and the metal corrodes along the grain boundaries while the surface may still look sound. This is intergranular corrosion, and steel in this susceptible condition is described as sensitized.
Welding heats a band of base metal beside every weld through that temperature range. How long the metal stays there decides whether damaging carbides form. At 0.030% maximum carbon there is too little carbon available to form a continuous carbide network in the time a normal weld thermal cycle takes, so the heat-affected zone of 304L keeps its corrosion resistance in the as-welded condition.
Welding is not the only way to sensitize stainless. Stress relieving a fabrication, hot forming, or heating a mixed carbon steel and stainless assembly for any reason can hold metal in the same range for minutes or hours rather than seconds. Low carbon grades tolerate those exposures far better, which is another reason heavy fabricators default to 304L.
When standard 304 is fine
- Thin sheet with single-pass welds, which cools through the sensitizing range in seconds
- Parts that will be solution annealed after welding, which dissolves any carbides that formed
- Service that is not corrosive enough to attack sensitized metal, such as dry indoor equipment
When a specification requires proof that material or welds are not susceptible, ASTM A262 describes the standard tests for detecting susceptibility to intergranular attack in austenitic stainless steels.
Welding thick sections and heavy fabrications
Heavy plate, multi-pass welds, high heat input processes and large weldments all keep more metal in the sensitizing range for longer. These are the jobs where 304L is specified by default, because solution annealing a large fabricated assembly after welding is usually impractical: it needs a furnace big enough for the part, rapid cooling, and often straightening afterward. Tanks, process vessels, structural frames, skids and heavy brackets fall into this group.
Weld 304L with ER308L filler metal so the deposit is also low carbon; ER308LSi is a common choice for MIG welding. The usual stainless practices apply: keep heat input and interpass temperature under control, expect more distortion than carbon steel because of higher thermal expansion, and remove heat tint where full corrosion resistance matters. ASA’s welding services cover manual welding and robotic weld cells for stainless assemblies.
Cutting and forming 304L
304L cuts, bends and machines the same way as 304. Its slightly lower yield strength can mean marginally less springback on the press brake, but bend allowances and tooling are generally interchangeable between the two. Fiber laser cutting with nitrogen assist leaves a clean, oxide-free edge that can be welded without grinding off scale.
Tip: 304L addresses sensitization caused by welding, not by long service at high temperature. For parts that operate for extended periods at elevated temperature and need strength there, designers often specify 304H, a separate grade with a controlled higher carbon range.
Dual-certified 304/304L
Much of the 304L produced today is dual certified as 304/304L. The material meets the 0.030% maximum carbon of 304L and also the 75 ksi (515 MPa) tensile and 30 ksi (205 MPa) yield minimums of 304, typically by using the nitrogen allowance (up to 0.10%) to recover the strength lost with carbon. One sheet or plate can then be used wherever either grade is called out.
Dual certification is shown on the mill test report, which lists both grades against the heat number. If your drawing requires 304L chemistry with 304 strength, say so on the purchase order and confirm it on the certification rather than assuming every 304L heat qualifies.
Choosing between 304, 304L and dual-certified material
| Situation | Usual choice |
|---|---|
| Thin sheet, short single-pass welds, mild service | 304 or 304L |
| Plate and heavy sections with multi-pass welds | 304L |
| Large weldments that cannot be annealed after welding | 304L |
| Welded parts that need 304 strength and 304L chemistry | Dual-certified 304/304L |
| Welded parts exposed to chlorides or salt | 316L |
Buying 304L stainless from ASA
ASA stocks 304L stainless alongside 304, 316 and 316L, with mill certifications and full material traceability available. For heavy welded parts, ASA can cut stainless plate up to 1.00 in thick on its CNC plasma plate cutting tables, then form and weld it in house. If your parts will see chlorides, compare 316L stainless steel before you request a quote.
Frequently asked questions
What is the difference between 304 and 304L?
The L stands for low carbon. Under ASTM A240, 304L is limited to 0.030% carbon versus 0.07% for 304, which prevents chromium carbide formation during welding. In exchange, its minimum tensile and yield strengths are each 5 ksi lower. In unwelded, annealed material the two grades resist corrosion essentially the same way.
Is 304L more corrosion resistant than 304?
Not in general. Both grades carry the same chromium and similar nickel, so in the annealed condition they resist corrosion equally. The advantage of 304L appears only after welding or other heating in the sensitizing range, where standard 304 may develop chromium-depleted grain boundaries that corrode while 304L stays resistant.
Can 304L be used where 304 is specified?
For corrosion resistance, yes, but plain 304L may not meet the 304 strength minimums of 75 ksi tensile and 30 ksi yield. Dual-certified 304/304L meets both the chemistry of 304L and the strength of 304, so it can usually substitute in either direction. Check the mill test report and any engineering approval your drawing requires.
Do I need 304L for thin sheet metal parts?
Often not. Thin gauge parts joined with short single-pass welds pass through the sensitizing temperature range quickly, so standard 304 usually performs well. 304L becomes the safer choice as sections get thicker, as weld passes multiply, or when the finished part will see an environment corrosive enough to attack any sensitized metal near the welds.
What filler metal is used for 304L?
ER308L is the standard filler for 304L. Its low carbon content matches the base metal, so neither the weld nor the surrounding heat-affected zone becomes prone to intergranular attack. ER308LSi, with added silicon, is popular for MIG welding because it improves puddle fluidity and bead wetting on stainless sheet and plate.