304 Stainless Steel: Properties, Composition and Uses

The chemistry, ASTM A240 properties, corrosion limits and fabrication behavior of 304 stainless steel, the most widely used stainless grade, plus how it compares with 304L and 316.

Updated October 2026 5 min read By the ASA team

On this page
  1. Chemical composition of 304 stainless steel
  2. Mechanical and physical properties
  3. Corrosion resistance of 304
  4. Welding and forming 304 stainless
  5. Common uses of 304 stainless steel
  6. 304 vs 304L and 316
  7. Buying 304 stainless from ASA

304 stainless steel is an austenitic chromium-nickel stainless steel containing roughly 18% chromium and 8% nickel, which is why it is often called 18-8 stainless. It is the most widely used stainless grade because it combines good corrosion resistance, excellent formability and weldability, and a nonmagnetic structure in the annealed condition.

Under ASTM A240, annealed 304 sheet, strip and plate must reach at least 75 ksi (515 MPa) tensile strength and 30 ksi (205 MPa) yield strength. This guide covers its chemistry, mechanical and physical properties, corrosion limits, fabrication behavior and where it fits against 304L and 316.

Chemical composition of 304 stainless steel

304 is designated UNS S30400 and is roughly equivalent to EN 1.4301. The table shows the chemistry limits ASTM A240 sets for flat-rolled 304.

ElementASTM A240 limit (wt%)
Carbon0.07 max
Manganese2.00 max
Silicon0.75 max
Phosphorus0.045 max
Sulfur0.030 max
Chromium17.5 to 19.5
Nickel8.0 to 10.5
Nitrogen0.10 max
IronBalance

Chromium is what makes 304 stainless: it forms a thin, self-repairing chromium oxide film that protects the surface. Nickel stabilizes the austenitic (face-centered cubic) structure, which gives 304 its toughness, ductility and lack of magnetism. The 0.07% carbon ceiling keeps the grade readily weldable in thin and moderate sections.

For flat-rolled product, ASTM A240 sets chemistry and mechanical properties, while ASTM A480 covers the general requirements that go with it: dimensional tolerances, flatness, surface finishes and testing. ASME SA240 and SA480 are the matching pressure vessel code versions. Naming the grade, the specification and the finish on the purchase order prevents substitution.

Some bar specifications and older references list 18.0 to 20.0% chromium and 0.08% maximum carbon for 304. Both describe the same grade; the specification named on your purchase order is the one that governs.

Mechanical and physical properties

Mechanical properties (annealed)

PropertyASTM A240 requirement
Tensile strength75 ksi (515 MPa) min
Yield strength (0.2% offset)30 ksi (205 MPa) min
Elongation in 2 in (50 mm)40% min
Hardness92 HRB (201 HBW) max

These are specification minimums, plus a hardness maximum. Mill test results usually exceed them, and the mill certification for each heat reports the measured values. 304 work hardens quickly, so cold rolling, bending and drawing raise its strength well above the annealed level. ASTM A666 covers annealed and cold-worked 304 for structural applications that need that higher strength.

Physical properties (typical)

PropertyTypical value
Density0.289 lb/in³ (8.00 g/cm³)
Modulus of elasticity28,000 ksi (193 GPa)
Mean thermal expansion, 32 to 212°F (0 to 100°C)9.6 µin/in·°F (17.3 µm/m·°C)
Thermal conductivity at 212°F (100°C)9.4 Btu/hr·ft·°F (16.3 W/m·K)
Electrical resistivity72 µΩ·cm
Melting range2550 to 2650°F (1400 to 1450°C)

Two of these numbers matter in the shop. 304 expands roughly half again as much as carbon steel when heated and conducts heat at roughly one third the rate, so heat stays concentrated near a weld or cut and parts distort more easily. Plan fixturing and weld sequences with that in mind.

Corrosion resistance of 304

304 resists atmospheric corrosion, fresh water, steam, most foods and beverages, many organic chemicals and oxidizing acids such as nitric acid. That range covers the majority of indoor and mild outdoor uses, which is why it is the default stainless grade.

Its weak point is chloride. Salt spray, seawater, deicing salt, and chlorinated cleaners or pool chemicals can break down the passive film locally and cause pitting and crevice corrosion. A common rule of thumb in water service limits 304 to roughly 200 ppm chloride at ambient temperature. Above about 140°F (60°C), chlorides combined with tensile stress can also cause stress corrosion cracking.

  • Good fit: indoor equipment, food contact surfaces, potable water, rural and most urban atmospheres.
  • Poor fit: coastal sites, splash zones, road salt exposure, brines and warm chloride solutions, where 316 is the better choice.
  • High temperature: 304 resists scaling in air to roughly 1600°F (870°C) in intermittent service and 1700°F (925°C) in continuous service (typical values).

Welding and forming 304 stainless

304 welds readily by TIG (GTAW), MIG (GMAW), stick (SMAW) and resistance methods, usually with ER308 or ER308L filler metal, and needs no preheat. The main risk is sensitization: when the heat-affected zone spends time in roughly the 800 to 1500°F (425 to 815°C) range, chromium carbides form at the grain boundaries and leave the steel open to intergranular corrosion. Thin sheet cools quickly enough that standard 304 is usually fine; heavy sections and multi-pass welds are where 304L stainless steel earns its place.

With 40% minimum elongation, 304 handles deep drawing, roll forming and tight press brake bends well. Expect more springback than carbon steel and higher forming loads, since the material strengthens as it bends. It machines more slowly than carbon steel for the same reason: sharp tools and steady feeds keep the cut below the work-hardened layer.

Tip: Keep carbon steel brushes, grinding wheels and fixtures away from 304. Embedded iron particles rust on the surface and make it look as if the stainless itself is corroding.

Common uses of 304 stainless steel

  • Food and beverage processing equipment, commercial kitchen tables, sinks and hoods
  • Tanks, hoppers and vessels for water and mild chemicals
  • Appliance panels and indoor architectural trim
  • Equipment enclosures, cabinets, brackets and frames for indoor service
  • Fasteners, springs and wire forms
  • Heat exchangers and exhaust components in moderate service

What these uses share is moderate exposure: clean water, food, indoor air or mild weather, with regular cleaning. Where parts face salt, brine or chlorinated chemicals, the same designs are usually built in 316 instead.

Finish matters as much as grade on visible and sanitary parts. A smoother finish is easier to clean and holds less dirt and salt residue, so put the finish on the drawing or purchase order next to the grade and specification.

304 vs 304L and 316

GradeWhat changesChoose it when
304Standard grade, 0.07% carbon maxGeneral fabrication, thin welded parts, indoor and mild outdoor service
304LCarbon limited to 0.030% max; slightly lower minimum strengthHeavy welded sections or weldments that cannot be annealed after welding
316Adds 2 to 3% molybdenum and more nickelChlorides, coastal and marine exposure, many chemical processes

For the details, see the guide to 316 stainless steel and the full 304 vs 316 stainless steel comparison, which covers cost, magnetism and a decision guide.

Buying 304 stainless from ASA

American Steel & Aluminum stocks 304 stainless as part of its stainless sheet and plate line, and its stock list references stainless specifications including ASTM A240, A480 and A666 and ASME SA240/SA480. Mill certifications and full material traceability are available. ASA can cut blanks on its 8 kW Trumpf fiber laser, form and weld them, and deliver from five Northeast locations, with most JIT orders delivered in 24 to 48 hours. Request a quote for 304 stainless with your size, quantity and specification.

Frequently asked questions

Is 304 stainless steel magnetic?

Annealed 304 is essentially nonmagnetic because its austenitic structure does not respond to a magnet. Cold working such as bending, rolling or deep drawing can convert part of that structure to martensite, so formed edges and corners may pull a magnet slightly. That mild attraction does not mean the material is the wrong grade or that its corrosion resistance has been lost.

Can 304 stainless steel be used outdoors?

Yes, in most inland settings. Rural and typical urban air leave 304 looking good for years with occasional washing. Near the ocean, in heavy industrial air or where road salt accumulates, chlorides cause brown surface staining and pitting on 304, and 316 is usually the better specification for those sites.

Is 18-8 stainless the same as 304?

18-8 describes a family of austenitic stainless steels with about 18% chromium and 8% nickel. 304 is the most common member, so the terms are often used interchangeably, especially for fasteners. Strictly, 18-8 can also include grades such as 302 and 305, so a drawing that needs 304 should name 304 and its governing specification.

Does 304 stainless steel rust?

304 resists rust in most everyday environments because chromium forms a protective oxide layer that reforms when scratched. It can still show rust-colored staining when chlorides break down that layer or when iron particles from carbon steel tools or grinding dust become embedded in the surface. Cleaning and passivation remove contamination; regular chloride exposure calls for 316.

What filler metal is used to weld 304 stainless?

ER308 and ER308L are the standard filler metals for joining 304 to itself, available as TIG rod and MIG wire. The L version keeps weld metal carbon low and is the more common choice today. Joining 304 to carbon steel usually calls for ER309L, whose higher alloy content tolerates dilution from the carbon steel side of the joint.

Material, processing and fabrication from one supplier

Send a drawing or a material list and the ASA team will quote it from stock.