On this page
1006, 1008 and 1010 steel are low carbon (mild) steels with no more than about 0.13% carbon, which makes them soft, very ductile and easy to weld. They are the workhorse grades for formed and drawn sheet metal parts, enclosures, panels, brackets and wire products, and they are the usual base metal for galvanized and other coated sheet.
The three grades differ mainly in carbon and manganese content, and therefore in strength and formability: 1006 is the softest and most formable, 1010 the strongest of the three. In sheet form they are usually bought to ASTM A1008 (cold rolled) or ASTM A1011 (hot rolled) commercial or drawing steel designations rather than by grade number alone.
Composition of 1006, 1008 and 1010
The grade numbers come from the AISI/SAE system: 10 means plain carbon steel, and the last two digits give the nominal carbon content in hundredths of a percent. SAE J403 sets these chemistry limits.
| Element (wt%) | 1006 | 1008 | 1010 |
|---|---|---|---|
| Carbon | 0.08 max | 0.10 max | 0.08 to 0.13 |
| Manganese | 0.45 max | 0.50 max | 0.30 to 0.60 |
| Phosphorus | 0.030 max | 0.030 max | 0.030 max |
| Sulfur | 0.050 max | 0.050 max | 0.050 max |
Older AISI tables list somewhat narrower manganese ranges for 1006 and 1008, and some purchase specifications still reference them. In practice the mill certification shows actual values, which typically sit well inside these limits.
For sheet, the ASTM designation matters more than the grade number. ASTM A1008 and A1011 commercial steel (CS) Type B allows 0.02 to 0.15% carbon, so 1008 and 1010 chemistries both qualify. Drawing steel (DS) Type B tightens carbon to 0.02 to 0.08% and requires the steel to be aluminum killed, which is why DS sheet is usually close to a 1006 chemistry.
Mechanical properties
Plain low carbon sheet has no mandatory strength minimums in its commercial and drawing steel designations. ASTM A1008 and A1011 list typical, nonmandatory ranges for guidance, shown below. If you need guaranteed strength, order a structural steel (SS) or high-strength low-alloy (HSLAS) designation instead.
| Product and designation | Typical yield strength | Typical elongation in 2 in |
|---|---|---|
| Cold rolled, A1008 CS | 20 to 40 ksi (140 to 275 MPa) | 30% or more |
| Cold rolled, A1008 DS | 22 to 35 ksi (150 to 240 MPa) | 36% or more |
| Hot rolled, A1011 CS | 30 to 50 ksi (205 to 340 MPa) | 25% or more |
| Hot rolled, A1011 DS | 30 to 45 ksi (205 to 310 MPa) | 28% or more |
For bar and heavier sections, 1010 is often quoted at a typical tensile strength of about 47 ksi (325 MPa) and yield of about 26 ksi (180 MPa) hot rolled, rising to roughly 53 ksi (365 MPa) tensile and 44 ksi (305 MPa) yield cold drawn. These are typical values only; actual results depend on size, processing and the mill.
Within the group, each step up in carbon and manganese adds a little strength and takes away a little ductility. The differences are modest: all three are far softer than 1045 medium carbon steel, and none can be meaningfully hardened by quenching.
Choosing between 1006, 1008 and 1010
| Grade | Strengths | Typical parts |
|---|---|---|
| 1006 | Lowest carbon, softest, best for deep drawing and severe forming | Deep drawn cups and housings, appliance shells, stamped panels with tight features |
| 1008 | The general-purpose sheet grade: excellent formability and weldability at a common price | Enclosures, electrical boxes, brackets, panels, shelving, ductwork, coating substrate |
| 1010 | Slightly stronger, still very formable; responds to carburizing | Structural brackets, fasteners and rivets, cold headed parts, case hardened components |
For most laser cut and press brake formed sheet metal, 1008 is the default, and many purchase orders read simply “C1008 cold rolled, commercial quality.” Choose 1006 or a DS designation when a part has deep draws or tight stretch forming that splits in CS. Choose 1010 when you want slightly more strength or plan to case harden.
Hot rolled vs cold rolled low carbon sheet
The same chemistry is sold in two very different products. Hot rolled sheet (ASTM A1011, and A1018 for heavier thicknesses) is finished at high temperature, has a gray-blue mill scale surface and looser thickness tolerances, and costs less. It can be supplied pickled and oiled, with the scale removed, for parts that will be painted or welded.
Cold rolled sheet (ASTM A1008) is further reduced at room temperature, then annealed and temper rolled. It has a smooth, clean surface, tighter thickness and flatness tolerances, and better consistency for precision forming. Thinner gauges are only made cold rolled. For gauge-to-thickness conversions, see the sheet metal gauge chart.
Low carbon steel as a coating substrate
Most hot-dip coated sheet starts as low carbon cold rolled or hot rolled steel of this type. Galvanized, galvannealed, Galvalume and aluminized products are ordered to their own coating specifications, such as ASTM A653 for zinc coatings, but the steel underneath behaves much like 1008 in forming and welding. The coating designation, such as G90, sets corrosion life, while the base metal designation (CS, DS or a structural grade) sets formability and strength. Our guide to galvanized steel covers the coating side.
Fabrication notes
Forming
Low carbon sheet bends to tight radii, often close to zero inside radius in thin cold rolled gauges, with little springback. One issue to watch is stretcher strain, also called Lüders lines: irregular bands that appear on the surface of formed parts made from steel that has aged after temper rolling. Aluminum killed drawing steel resists aging, and fresh material or roller leveling just before forming also helps on exposed surfaces.
Welding
All three grades weld easily by MIG, TIG, spot and projection welding without preheat. Low carbon means the heat-affected zone does not harden, so cracking is rarely a concern. For galvanized versions, remove or ventilate the zinc coating at the weld.
Machining and heat treatment
Low carbon steels machine poorly compared with their softness: they are gummy, build up on cutting edges and form long stringy chips. Free machining grades are better for turned parts. Quenching does not harden these steels in any useful way, but 1010 and similar grades are often carburized, which adds carbon to the surface so it can be case hardened over a soft, tough core.
Tip: If a formed part needs a guaranteed yield strength, specify it. A plain CS or DS order is not tested for strength, so two shipments can form and spring back differently. An SS or HSLAS designation, or a tighter forming steel class, gives you control.
Buying low carbon steel from ASA
American Steel & Aluminum stocks C1006, C1008 and C1010 among the hot rolled and cold rolled carbon steels in its flat rolled sheet and plate line, with stock list specifications including ASTM A1008, A1011, A1018 and A568. Its Alcos 6-high leveling and cut-to-length line processes carbon steel from 24 to 11 gauge in widths of 14 to 72 in, and ASA can laser cut and press brake form the blanks into finished parts. Most JIT orders are delivered in 24 to 48 hours.
Frequently asked questions
Is 1008 steel the same as mild steel?
1008 is one type of mild steel. Mild steel is an informal term for low carbon steels, generally below about 0.25% carbon, so it covers 1006, 1008, 1010, 1018, A36 and others. When someone asks for mild steel sheet, they usually mean a low carbon commercial steel such as 1008 or 1010, but the order should name the specification.
What is the difference between C1008 and 1008?
None in chemistry. The C prefix is an older AISI convention that originally marked basic open hearth carbon steel, and it survives on many stock lists and purchase orders. C1008, 1008 and SAE 1008 all refer to the same grade. What matters more for sheet is the ASTM designation, such as A1008 CS Type B.
Can 1010 steel be hardened?
Not by simple quenching. With roughly 0.10% carbon, 1010 does not form enough martensite to become hard. It can be surface hardened by carburizing or carbonitriding, which diffuse carbon or carbon and nitrogen into the surface before quenching. That produces a hard, wear resistant case over a soft core, common for pins, small gears and bushings.
Which low carbon steel is best for deep drawing?
Lower carbon and aluminum killing give the best drawing performance, so 1006 chemistry in an ASTM A1008 drawing steel (DS) designation is the usual choice. For very severe draws, deep drawing steel (DDS) and extra deep drawing steel (EDDS) designations go further, with even lower carbon and interstitial control. Commercial steel suits ordinary bending and moderate forming.
Is 1008 steel good for welding?
Yes. Its very low carbon and manganese give a low carbon equivalent, so it welds by MIG, TIG, spot, seam and projection methods without preheat, and the heat-affected zone stays ductile. Clean the surface of oil before welding. Hot rolled material with mill scale welds better after pickling or grinding, especially for appearance-critical welds.