On this page
In shipbuilding, marine-grade steel usually means hull structural steel made to classification society rules such as ABS Grade A or AH36, or to ASTM A131, while marine-grade aluminum means 5xxx series aluminum-magnesium alloys such as 5083, 5086 and 5456 that resist seawater corrosion and keep good strength when welded. “Marine grade” is not a single specification: it describes materials qualified for the loads, temperatures and corrosion conditions of service at sea.
Most large commercial and naval ships are steel. Aluminum is common in fast ferries, patrol boats, workboats and many superstructures, where lighter weight pays back in speed, payload and fuel. Many vessels use both.
What makes a material marine grade
A material earns the label by meeting requirements that go beyond a general structural grade:
- Notch toughness. Hull steel has to resist brittle fracture in cold water and under impact, so most grades are qualified with Charpy V-notch tests at set temperatures.
- Weldability. Ship structure is welded, so chemistry is controlled to limit hardening and cracking in the heat-affected zone.
- Corrosion behavior. Aluminum alloys for hulls are tested for resistance to exfoliation and intergranular attack; steels rely on coatings and cathodic protection.
- Certification. Plate and shapes for classed vessels are typically produced and tested under the rules of a classification society such as ABS, DNV or Lloyd’s Register, often with a surveyor’s witness and stamp on the mill certificate.
Builders should confirm what the vessel’s class rules, the owner’s specification or the government contract require, because the same nominal grade can be sold with or without class certification.
Marine steel grades at a glance
Hull structural steels are grouped by strength level, with a letter that indicates the impact test temperature. ASTM A131 uses the same grade designations as the classification societies.
| Group | Grades | Minimum yield strength |
|---|---|---|
| Ordinary strength | A, B, D, E | 34 ksi (235 MPa) |
| Higher strength, 32 level | AH32, DH32, EH32, FH32 | 46 ksi (315 MPa) |
| Higher strength, 36 level | AH36, DH36, EH36, FH36 | 51 ksi (355 MPa) |
| Higher strength, 40 level | AH40, DH40, EH40, FH40 | 57 ksi (390 MPa) |
Moving from A to B, D, E and F means impact testing at progressively colder temperatures, which is why D and E grades show up in ice service, cold-region vessels and highly stressed areas. Naval combatants add specialized high-strength steels such as HY-80 and HSLA-80 made to military specifications. Grade selection, thickness and processing are covered in more depth in our guide to steel plate for shipbuilding.
Marine aluminum alloys
The 5xxx series gets its strength from magnesium and from strain hardening, not heat treatment. That matters at sea: welding does not wipe out a precipitation-hardened structure the way it can in heat-treatable alloys, and magnesium gives good resistance to seawater.
| Alloy | Magnesium (Aluminum Association range) | Typical marine uses |
|---|---|---|
| 5052 | 2.2 to 2.8% | Small boat hulls, tanks, hatches, interior and superstructure parts |
| 5086 | 3.5 to 4.5% | Hull plating and structure on workboats and patrol craft |
| 5083 | 4.0 to 4.9% | Hull and deck plating on larger aluminum vessels |
| 5456 | 4.7 to 5.5% | Higher-strength hull plate, often in naval and high-speed craft |
For hull plate, the key specification is ASTM B928, which covers high-magnesium 5xxx sheet and plate for marine service in the H116 and H321 tempers. Material to B928 is tested for resistance to exfoliation and intergranular corrosion, using methods such as ASTM G66 and ASTM G67. General-purpose 5xxx sheet ordered only to ASTM B209 may not include the same corrosion testing, so check that the order calls for B928 where the design requires it.
Extruded stiffeners, frames and deck planks on aluminum vessels are often 6xxx series alloys. These are heat treatable, so they lose a meaningful share of their strength next to welds, and designers account for that reduced heat-affected zone strength when sizing members and placing joints. Fasteners, castings and fittings bring in still more alloys, which is one reason a material list for an aluminum vessel deserves careful review.
5052 has less magnesium and lower strength than the hull alloys, but it forms easily, welds well and resists corrosion, which makes it a long-standing choice for small craft, tanks and outfitting. Our guide to 5052 aluminum covers its tempers and properties.
Tip: Alloys with more than about 3% magnesium can become sensitized after long exposure to elevated temperatures, often cited as about 150 F (65 C) and above, which makes them prone to intergranular corrosion and cracking. Keep high-magnesium plate away from engine rooms, exhaust runs and other hot spots unless the alloy and temper are qualified for it.
Steel vs aluminum for hulls and structure
The choice is a trade-off between weight, stiffness, cost and how the vessel will be built and maintained.
| Factor | Steel | Aluminum (5xxx) |
|---|---|---|
| Density | About 0.284 lb/in³ (7.85 g/cm³) | About one third of steel |
| Stiffness (modulus) | About 29,000 ksi (200 GPa) | About 10,000 ksi (69 GPa), so more depth or framing is needed |
| Welding | Forgiving, widely practiced, high productivity | Clean conditions, specialized procedures; strength drops in the heat-affected zone of strain-hardened tempers |
| Corrosion | Needs coatings and cathodic protection | Good natural resistance; sensitive to galvanic contact |
| Fire | Keeps strength at higher temperatures | Loses strength at much lower temperatures; insulation is often required |
| Material cost | Lower per pound | Higher per pound, partly offset by lower weight |
A common compromise is a steel hull with an aluminum superstructure, which lowers the center of gravity and topside weight. The joint between the two is usually made with explosion-bonded transition strips or bolted connections with insulation to prevent galvanic corrosion. Our broader comparison of aluminum vs steel covers the properties behind these differences.
Stainless steel and galvanic corrosion
Stainless steel appears throughout a vessel in fittings, railings, hardware, galley equipment and tanks. 316 and 316L are the usual marine choices because molybdenum improves resistance to chlorides; 304 is generally kept to interiors and areas that see only occasional spray. Even 316 can suffer crevice and pitting corrosion in stagnant seawater, so it is not automatically suitable for immersion.
Whenever two different metals touch in seawater, the less noble one corrodes faster. Aluminum and zinc-coated steel sit on the active end of the galvanic series, while stainless steel and copper alloys are more noble. Designers break the circuit with insulating washers, sleeves, gaskets and sealants, avoid small aluminum parts fastened with large stainless areas, and use sacrificial anodes to protect hulls and appendages.
Marine and defense materials from ASA
American Steel & Aluminum supports shipbuilding and defense programs with DFARS-compliant domestic steel, split and bulb tees and heavy plate processing, and stocks 304, 304L, 316 and 316L stainless and 5052 aluminum for outfitting, tanks and fabricated parts. Our West Bath, ME facility handles tee and beam processing and plate work, with mill certifications, full material traceability and just-in-time delivery. Where a drawing calls for class-certified hull steel or ASTM B928 aluminum plate, state that on the request for quote so availability and certification can be confirmed before ordering. Read more about our shipbuilding and defense fabrication services.
Frequently asked questions
Is 5052 aluminum marine grade?
5052 is widely used in marine applications and resists seawater well, especially for small boat hulls, fuel and water tanks, hatches and outfitting. It is not one of the high-magnesium hull plate alloys covered by ASTM B928, such as 5083, 5086 and 5456, so larger vessels and classed hull structures usually call for those alloys in H116 or H321 temper.
What is the difference between AH36 and A36?
AH36 is a ship plate grade made to ASTM A131 or classification society rules, with a 51 ksi minimum yield and Charpy impact testing. A36 is a general structural steel under ASTM A36 with a 36 ksi minimum yield and no impact test requirement in the base specification. They are not interchangeable on classed vessels.
What does H116 temper mean for marine aluminum?
H116 is a strain-hardened temper used for 5xxx alloys with at least 3% nominal magnesium that has been specially processed and tested for resistance to exfoliation and intergranular corrosion. Together with H321, it is the temper usually specified for hull plate under ASTM B928. Standard H32 or H34 tempers do not carry those corrosion tests.
Why is stainless steel not always safe below the waterline?
Stainless steel relies on a thin oxide film that needs oxygen to repair itself. In stagnant seawater, under fouling, gaskets or tight joints, oxygen runs out and chlorides can break down the film, causing crevice and pitting corrosion. Even 316 can be affected, so immersed parts need careful design, regular flow or a more resistant alloy.
Do shipbuilding materials need class society certification?
For vessels built to class, yes: hull structural steel and aluminum are usually produced and tested under the rules of a classification society such as ABS, DNV or Lloyd's Register, with certified mill reports. Naval vessels are governed by Navy specifications and contract requirements, which may also invoke class rules. Uncertified material of the same nominal grade may not be accepted, so state the certification requirement on the order.