On this page
Stainless steel and aluminum both weld well, but for nearly opposite reasons they need different handling. Stainless steel holds heat in a small area, so the main risks are distortion, heat tint and loss of corrosion resistance. Aluminum pulls heat away quickly and is covered by a high-melting oxide, so the main challenges are oxide removal, porosity and a loss of strength next to the weld.
Understanding those differences helps engineers design better joints and helps buyers know what to ask a fabricator. This guide compares the two metals using 304 stainless and 5052 aluminum as the reference alloys, since both are common choices for welded sheet and plate parts.
Key differences at a glance
The physical properties below are typical published values for annealed 304 stainless and 5052 aluminum. They explain most of the welding behavior that follows.
| Property (typical) | 304 stainless | 5052 aluminum |
|---|---|---|
| Melting range | About 2,550 to 2,650 °F (1,400 to 1,450 °C) | About 1,125 to 1,200 °F (607 to 649 °C) |
| Thermal conductivity | About 9.4 BTU/hr·ft·°F (16 W/m·K) | About 80 BTU/hr·ft·°F (138 W/m·K), roughly 8.5 times higher |
| Thermal expansion | About 9.6 µin/in·°F (17.3 µm/m·°C) | About 13.2 µin/in·°F (23.8 µm/m·°C) |
| Surface oxide | Thin chromium oxide; protects the metal | Aluminum oxide melting near 3,760 °F (2,070 °C) |
| Main welding risks | Distortion, heat tint, sensitization | Lack of fusion, porosity, cracking, HAZ softening |
| Typical filler | ER308L (304, 304L), ER316L (316, 316L) | ER5356 or ER4043, depending on alloy and use |
| Structural welding code | AWS D1.6 | AWS D1.2 |
Two numbers stand out. Aluminum conducts heat about 8.5 times faster than 304, so it needs more heat input to start a puddle and cools quickly once the arc moves on. Stainless conducts heat poorly but expands more than carbon steel, so heat stays concentrated near the joint and pulls the part out of shape as it cools.
Welding stainless steel: what matters
Heat control and distortion
Because stainless keeps heat near the weld, long seams on thin sheet bow and buckle easily. Fabricators control this with lower heat input, short stitch welds, balanced weld sequences, copper or aluminum backing bars that draw heat away, and fixtures. Overwelding, meaning welds larger than the design requires, is a common cause of distortion and should be avoided on the drawing.
Sensitization and L grades
When austenitic stainless spends time between roughly 800 and 1,500 °F (425 and 815 °C), chromium can combine with carbon to form chromium carbides at grain boundaries. The metal next to the weld then has less free chromium and can corrode along those boundaries. Low-carbon L grades such as 304L and 316L, and fillers such as ER308L and ER316L, reduce this risk. See 304 vs 304L stainless steel for when the L grade is worth specifying. Many procedures also cap interpass temperature, often around 350 °F (175 °C), to limit time in that range.
Heat tint, purging and cleanup
The straw, blue and gray colors next to a stainless weld are oxide layers that reduce corrosion resistance. They are removed by mechanical cleaning, pickling paste or electrochemical cleaning, often followed by passivation. Full penetration welds on tube or sanitary parts usually need an argon back purge so the root side does not oxidize.
Contamination
Carbon steel particles embedded in stainless will rust and stain the surface. Shops use dedicated stainless brushes, grinding wheels and clamps, and keep stainless work separated from carbon steel grinding.
Welding aluminum: what matters
Oxide removal and cleanliness
Aluminum oxide melts at about three times the temperature of the base metal. If it is not removed, it traps unfused metal and inclusions. TIG welding on alternating current breaks up the oxide during each cycle, while MIG welding relies on the cleaning action of the arc with the wire as the positive electrode. Joints are cleaned with a solvent to remove oil, then brushed with a dedicated stainless steel brush shortly before welding, because the oxide starts to rebuild immediately.
Porosity
Hydrogen is the main cause of porosity in aluminum welds. It comes from moisture, oil, hydrated oxide and contaminated filler wire. Dry, clean material and filler, good gas coverage and proper storage of wire spools prevent most porosity problems.
Heat input and cracking
High conductivity means aluminum often needs more current than steel of the same thickness, and thick sections may be preheated. Aluminum also shrinks significantly as it solidifies, so the crater at the end of a weld can crack if it is not filled. Welders use crater fill settings or reverse briefly at the end of each bead.
Strength loss in the heat-affected zone
Strain-hardened alloys such as 5052-H32 get their strength from cold work, and welding heat anneals the metal next to the weld. That zone falls toward O temper strength. ASTM B209 lists a minimum tensile strength of 31 ksi (215 MPa) for 5052-H32 and 25 ksi (170 MPa) for 5052-O, so designers of welded aluminum parts typically base weld zone strength on the annealed values. Our 5052 aluminum guide covers the alloy’s tempers.
Filler selection
ER5356 is the usual filler for 5052 and other 5xxx alloys, giving higher weld strength. ER4043 flows more easily, is less prone to some cracking problems and suits many other alloys, but it turns dark gray when anodized, so ER5356 is the better color match on parts that will be anodized.
Tip: On welded aluminum assemblies, put welds in lower-stress areas where you can, and size the part using the weld zone strength rather than the temper strength of the sheet.
Process choices for each metal
Both metals are commonly welded with TIG and MIG, but the setup differs. The general tradeoffs between the two processes are covered in MIG vs TIG welding.
| Process | Stainless steel | Aluminum |
|---|---|---|
| TIG (GTAW) | Direct current, argon shielding; standard for thin sheet and visible welds | Alternating current for oxide cleaning, argon or argon-helium shielding |
| MIG (GMAW) | Argon-rich gases blended for stainless; short circuit, spray or pulsed transfer | Argon or argon-helium, spray or pulsed transfer; spool gun or push-pull feeder for soft wire |
| Robotic MIG | Common for production brackets, frames and enclosures | Common with pulsed MIG and push-pull wire feed |
| Post-weld work | Heat tint removal, pickling or passivation | Brushing; finishing as required by anodize or coating |
Welding procedure specifications should be qualified for the specific alloy, thickness and process. Structural work typically follows AWS D1.6 for stainless steel and AWS D1.2 for aluminum.
Joining stainless steel to aluminum
Stainless steel and aluminum cannot be reliably joined by conventional arc welding. The two metals form brittle intermetallic compounds in the weld, and the melting points are more than 1,300 °F (700 °C) apart. Practical options include:
- Mechanical fasteners, rivets or clinching, with an insulating barrier to limit galvanic corrosion
- Bimetallic transition inserts made by explosion bonding, so each side is welded to its matching metal
- Structural adhesives, where the load and service temperature allow
Whenever the two are in contact in a wet environment, aluminum is the anode and will corrode preferentially. Isolating washers, sealants and coatings reduce the risk.
Welding stainless and aluminum at ASA
Welding at ASA covers carbon steel, stainless and aluminum, using manual welding stations alongside robotic weld cells for production runs. Assemblies and weldments can be built from stainless and aluminum that ASA stocks, including 304, 304L, 316, 316L and 430 stainless and 3003-H14, 5005 and 5052 aluminum, with cutting, forming and welding handled under one company. See welding for more.
Frequently asked questions
Is aluminum harder to weld than stainless steel?
Most welders find aluminum less forgiving. Its oxide must be removed, it conducts heat away quickly, it shows little color change before melting and it is prone to hydrogen porosity. Stainless is easier to puddle but punishes excess heat with distortion and heat tint. Both weld well with qualified procedures, clean material and the correct filler metal.
What filler metal is used for 304 stainless and 5052 aluminum?
For 304 and 304L stainless, ER308L is the standard choice, and ER316L is used for 316 and 316L. For 5052 aluminum, ER5356 is the common filler because it gives higher weld strength and a better color match after anodizing. ER4043 is easier to feed and flows well, and it is widely used on other aluminum alloys.
Does welding weaken aluminum?
In strain-hardened and heat-treated alloys, yes. Welding heat anneals the metal beside the weld, so a 5052-H32 part drops toward O temper strength in the heat-affected zone. ASTM B209 minimum tensile strength is 31 ksi for 5052-H32 versus 25 ksi for 5052-O, so welded aluminum structures are designed around the reduced strength.
Why does stainless steel change color when welded?
The colors are heat tint, thin oxide layers that form when hot stainless contacts air. They range from straw to blue to gray as temperature rises. Heat tint lowers the corrosion resistance of the surface, so it is removed by brushing, grinding, pickling or electrochemical cleaning, then often passivated, especially on parts exposed to moisture or chemicals.
Can you weld stainless steel to aluminum?
Not with conventional arc welding. The metals form brittle intermetallic compounds and their melting points are far apart, so the joint cracks. Common alternatives are bolts or rivets with an insulating barrier, explosion-bonded transition inserts that let each side be welded to its own metal, or structural adhesives where loads and temperatures allow.