On this page
Powder coating is a dry finishing process in which electrostatically charged powder (finely ground resin, pigment and additives) is sprayed onto a grounded metal part and then cured in an oven, where it melts and cross-links into a continuous film. The result is a hard, uniform finish, typically 2 to 4 mils (50 to 100 µm) thick, that resists chipping, abrasion and corrosion better than most conventional liquid paints.
How long that finish lasts depends less on the powder itself than on pretreatment, chemistry selection and part design. This guide covers each step, the main powder chemistries, how durability is tested and what drives cost.
The powder coating process step by step
1. Pretreatment
Powder sticks only as well as the surface beneath it. Oil, mill scale, rust, weld spatter and laser oxide all have to go. Most lines use one or both of these approaches:
- Chemical pretreatment: an alkaline cleaning stage, rinses and a conversion coating such as iron phosphate, zinc phosphate or a zirconium-based treatment. The conversion coating improves adhesion and slows corrosion that starts at scratches.
- Abrasive blasting: removes mill scale and rust from hot rolled steel and weldments and creates a surface profile the coating can grip. Blasting is the usual choice for heavy fabrications and hot rolled material.
Aluminum needs its own conversion coating, since the natural oxide layer does not give powder a reliable anchor. Galvanized steel is coatable, but zinc can release trapped gas during cure and leave pinholes, so it is often preheated to outgas before coating or sprayed with an outgassing-tolerant powder.
2. Electrostatic application
The part hangs on a grounded rack while a spray gun gives the powder particles an electrostatic charge. The charged particles wrap around edges and cling to the part until cure. Overspray that misses the part can be collected and reused on many systems, which is one reason powder wastes far less material than liquid paint.
The electrostatic field has one weakness: the Faraday cage effect. The electric field concentrates on edges and openings, so powder struggles to reach deep inside corners, narrow channels and recesses. Those areas come out thin unless the operator adjusts gun settings or touches them up manually.
3. Curing
In the cure oven, the powder flows out into a smooth film and chemically cross-links. A typical schedule is about 10 minutes at 400 °F (204 °C) or 20 minutes at 350 °F (177 °C), measured at part temperature rather than air temperature. Schedules vary by powder, so the cure window on the manufacturer’s technical data sheet governs. Heavy weldments take longer to come up to temperature than thin sheet, and under-cured parts look fine but fail adhesion and solvent tests.
Film thickness
A single coat of powder typically measures 2 to 4 mils (50 to 100 µm). Textured finishes run thicker, and two-coat systems with a primer and topcoat often reach 4 to 8 mils (100 to 200 µm). Dry film thickness is checked with a magnetic or eddy current gauge, following methods such as ASTM D7091.
Thicker is not automatically better. Excess film can chip at edges, interfere with fits and cause orange peel. Remember that a coated hole shrinks by twice the film thickness, so specify masking or oversize holes and slots that receive fasteners or mating parts.
Powder coating chemistries
Powders are grouped by resin chemistry. Choosing the right one for the service environment matters more than any other specification on the drawing.
| Chemistry | Strengths | Limitations | Typical use |
|---|---|---|---|
| Epoxy | Excellent adhesion, chemical and corrosion resistance | Chalks and fades in sunlight | Indoor equipment, primers under exterior topcoats |
| Hybrid (epoxy-polyester) | Good finish, lower cost, tolerant of overbake | Limited UV resistance | Indoor enclosures, racks, fixtures, shelving |
| Polyester (TGIC and TGIC-free) | Good UV and weather resistance, good mechanical properties | Less chemical resistance than epoxy | Outdoor equipment, frames, general exterior parts |
| Urethane polyester | Smooth thin films, good chemical and weather resistance | Can be harder to apply thick | Appliance and equipment panels |
| Super durable polyester | Extended gloss and color retention outdoors | Higher cost than standard polyester | Architectural and long-life outdoor parts |
For harsh outdoor or coastal exposure, a common approach is a zinc-rich or epoxy primer under a polyester or super durable topcoat. The primer protects the steel and the topcoat protects the primer from UV.
Durability and salt spray testing
The most widely cited corrosion test is ASTM B117, a neutral salt spray (fog) test in which scribed panels sit in a 5% sodium chloride fog at 95 °F (35 °C). Results are reported as the number of hours a coating survives before reaching a set amount of blistering or creep from the scribe. Specifications commonly ask for 500, 1,000 or more hours depending on the system and service.
Salt spray hours are useful for comparing coating systems and controlling quality, but they do not convert directly into years of field life. Real environments cycle through wet and dry, UV and temperature, so many buyers pair ASTM B117 with other checks:
- Adhesion: crosshatch tape test per ASTM D3359
- Hardness: pencil hardness per ASTM D3363
- Impact resistance: falling weight test per ASTM D2794
- Weathering: accelerated UV or outdoor exposure for gloss and color retention
Pretreatment has the largest effect on salt spray results. The same powder over a zinc phosphate or blasted and primed surface will typically outperform it over a simple cleaned surface by a wide margin.
Powder coating vs liquid paint
| Factor | Powder coating | Liquid paint |
|---|---|---|
| Film per coat | 2 to 4 mils (50 to 100 µm) in one pass | Often multiple coats for the same build |
| Toughness | High chip and abrasion resistance | Varies widely by system |
| VOCs | Near zero; no solvents | Solvent-borne systems emit VOCs |
| Material use | Overspray can be reclaimed | Overspray is lost |
| Limits | Needs a cure oven; heat-sensitive parts excluded; field touch-up is harder | Air dry or low bake possible; easy to touch up |
Cost drivers and design tips
Powder coating is usually priced by the part or by the rack, and the biggest cost drivers are labor rather than powder:
- Surface area and size: large parts limit how many fit on a rack and in the oven.
- Racking density: parts that hang easily and nest closely cost less per piece.
- Masking: every plug, cap and taped surface is manual labor.
- Pretreatment level: blasting, multi-stage chemical treatment and primers add steps.
- Color and batch size: custom colors, special effects and frequent color changes add setup and cleanup time.
- Part mass: heavy weldments need longer cure cycles.
These design choices improve finish quality and lower the price:
- Add racking holes in non-cosmetic locations so parts can hang without contact marks on visible faces.
- Call out masking clearly: threads, bearing and mating surfaces, ground points and holes that receive fasteners.
- Break or radius sharp edges, because powder pulls thin on knife edges and that is where corrosion starts.
- Vent closed tube sections and weldments so pretreatment solutions drain and trapped air can escape during cure.
- Avoid deep, narrow recesses that create Faraday cage problems, or accept a lighter film there.
- Remove weld spatter and grind welds that will be visible, since powder telegraphs every surface defect (see MIG vs TIG welding).
Tip: Specify color by a standard code (RAL or a powder manufacturer’s product number), along with gloss level and texture. “Black” on a drawing can mean a dozen different finishes. For coated substrates, see our guide to galvanized steel.
Powder coating at ASA
ASA powder coats parts and welded assemblies, and the Auburn, MA facility has both blasting and powder coating, so parts can move from cutting and forming through welding and finishing under one company. See powder coating for details, or request a quote with your drawings and finish specification.
Frequently asked questions
How thick is a powder coat finish?
A single powder coat typically measures 2 to 4 mils (50 to 100 µm), about the thickness of a sheet of paper. Textured powders build thicker, and two-coat systems with a primer and topcoat often reach 4 to 8 mils (100 to 200 µm). Excessive thickness can chip at edges and interfere with holes, threads and mating parts.
Is powder coating better than paint?
For most metal parts, yes. Powder coating builds a thicker, tougher film in one pass, releases almost no solvents and lets overspray be reclaimed. Liquid paint is still the better fit for heat-sensitive assemblies, very large structures that will not fit in an oven, very thin films and finishes that need easy touch-up in the field.
Can you powder coat galvanized steel and aluminum?
Yes, with the right preparation. Aluminum needs a conversion coating so the powder bonds to a stable, uniform surface rather than the thin, variable natural oxide. Galvanized steel can release gas from the zinc layer during cure, causing pinholes, so it is commonly preheated to outgas or coated with a powder formulated to tolerate outgassing.
What does 1,000 hours of salt spray mean?
It means coated test panels, usually scribed through to the metal, survived 1,000 hours in an ASTM B117 neutral salt fog before exceeding a set limit of blistering or corrosion creep. It is a useful way to compare coating systems and check consistency, but it does not translate directly into a number of years outdoors.
How can I reduce the cost of powder coating parts?
Design parts that hang easily with racking holes in hidden spots, minimize masking, use standard colors and group parts into larger batches of the same color. Venting closed sections and removing sharp edges and weld spatter before coating also cut rework. Clear finish callouts on the drawing prevent quoting and production delays.