On this page
MIG welding is faster and less expensive per inch of weld, which makes it the standard choice for production work on carbon steel and for thicker sections of stainless and aluminum. TIG welding is slower and more skill-intensive, but it gives the most control, the cleanest appearance and the best results on thin material and visible joints.
Most fabricated assemblies do not need one process exclusively. The practical question is which process suits each joint, given the material, thickness, appearance requirements and how many parts you need.
How MIG and TIG welding work
MIG (GMAW). Gas metal arc welding feeds a continuous solid wire electrode through the gun. The arc forms between the wire and the workpiece, the wire melts into the joint as filler, and shielding gas from the nozzle protects the molten pool. Because the welder only guides the gun and the machine feeds the wire, MIG is quick to learn and easy to automate.
MIG can run in several metal transfer modes. Short-circuit transfer suits thin sheet and out-of-position welds, while spray and pulsed spray transfer deliver higher deposition and deeper fusion on thicker material.
TIG (GTAW). Gas tungsten arc welding uses a non-consumable tungsten electrode to create the arc. The welder adds filler rod separately by hand and usually controls amperage with a foot pedal, while pure argon shields the weld. Having heat input and filler in separate hands gives TIG its precision, and also makes it slower.
MIG vs TIG welding comparison
| Factor | MIG (GMAW) | TIG (GTAW) |
|---|---|---|
| Electrode | Consumable wire, continuously fed | Non-consumable tungsten plus separate filler rod |
| Travel speed and deposition | High; typically several times manual TIG | Low |
| Best thickness range | About 18 ga (1.2 mm) sheet through heavy plate, multipass on thick sections | Thin gauge sheet to medium sections; excels below about 1/8 in (3.2 mm) |
| Appearance | Good; some spatter, often cleaned or ground | Excellent; no spatter, fine ripple bead |
| Heat control | Set by machine parameters | Adjusted continuously by the welder |
| Surface prep needed | More tolerant of mill scale and minor contamination | Requires clean metal |
| Operator skill | Moderate | High |
| Automation | Widely used in robotic cells | Possible, less common |
| Cost per inch | Lower | Higher |
Speed, quality and cost
Speed is MIG’s biggest advantage. As typical ranges, manual TIG deposits roughly 0.5 to 2 lb (0.2 to 0.9 kg) of weld metal per hour, while semiautomatic MIG commonly deposits about 3 to 12 lb (1.4 to 5.4 kg) per hour, depending on wire size and transfer mode. On long seams and large weldments, that difference dominates labor cost.
TIG wins on control and appearance. The welder can add heat and filler independently, which makes it easier to weld thin edges without burning through, fuse outside corners cleanly and produce a consistent bead on cosmetic stainless or aluminum. TIG also produces no spatter, so there is less cleanup before finishing.
Quality is not the same as appearance. A properly set up MIG weld on carbon steel is fully as strong as a TIG weld, and AWS D1.1 (structural steel) accepts both processes. D1.1 prequalifies MIG in spray, globular and pulsed spray transfer, while short-circuit MIG and TIG need welding procedures qualified by testing. Choose TIG for strength only when the joint geometry or material makes MIG hard to control.
Thickness
On sheet thinner than about 18 ga (1.2 mm), TIG usually gives better results because heat can be eased off precisely at edges and corners. From about 1/8 in (3.2 mm) up, MIG becomes the more efficient option, and on plate it is the clear choice, with multipass welds on thick sections. Many shops TIG weld the root of a critical joint and fill it with MIG to combine control with speed.
Tip: Weld quality starts with fit-up. Accurately laser cut and press brake formed parts leave consistent gaps, which reduces filler use, distortion and rework with either process.
Steel, stainless and aluminum considerations
Carbon steel
MIG is the default for carbon steel frames, brackets, structural assemblies and equipment bases. Common practice is ER70S-6 wire with a 75% argon and 25% CO2 shielding gas. MIG tolerates light mill scale better than TIG, though hot rolled steel still welds best after the joint area is cleaned. On galvanized steel, the zinc coating near the joint is usually removed first because it causes porosity and hazardous fumes.
Stainless steel
Both processes work well on stainless. TIG is preferred for thin sheet, sanitary-looking joints and visible welds, while MIG with a stainless wire such as ER308L or ER316L and a stainless-specific gas blend handles heavier sections faster. Low-carbon L grades such as 304L and 316L are often specified for welded parts because they resist carbide precipitation in the heat-affected zone.
Heat tint, the straw to blue discoloration next to a stainless weld, reduces corrosion resistance. It is removed by mechanical cleaning or pickling, and full penetration welds often need an argon back purge to protect the root side.
Aluminum
Aluminum conducts heat quickly and is covered by an oxide that melts at about 3,760 °F (2,070 °C), far hotter than the metal underneath at about 1,220 °F (660 °C). TIG welding on alternating current breaks up that oxide during the cleaning half of the cycle, giving excellent control on thin aluminum sheet. MIG on aluminum uses 100% argon, spray or pulsed transfer and a spool gun or push-pull feeder because soft aluminum wire buckles in a standard liner. It is much faster on thicker sections.
Filler choice matters. ER5356 is a common match for 5052 and other 5xxx alloys, while ER4043 flows more easily and is widely used on other alloy families. Clean aluminum with a solvent and a dedicated stainless steel brush just before welding.
Robotic MIG welding for production
For repeat parts, robotic MIG welding is the most efficient option. A robot holds torch angle, travel speed and wire stick-out constant on every part, which delivers consistent bead size and penetration across a run, and it keeps the arc on far longer per shift than a manual welder can.
Robotic welding pays off when:
- The part runs in production quantities, so fixture and programming costs spread across many pieces.
- Component parts are cut and formed consistently, so joints land where the program expects them.
- The design gives the torch clear access to each joint.
- Weld size and appearance need to match from the first part to the last.
Prototypes, one-off weldments, very large assemblies and cosmetic TIG work still belong at manual welding stations. Many programs start manual and move to a robotic cell once the design is stable and volumes grow.
Welding at ASA
ASA welds carbon steel, stainless and aluminum at manual welding stations and in robotic weld cells for production runs, producing welded assemblies and weldments as part of its industrial equipment and OEM contract manufacturing. Parts can be cut, formed, welded and powder coated under one company. Visit welding for more on ASA’s capabilities.
Frequently asked questions
Is TIG welding stronger than MIG welding?
Not inherently. A properly qualified MIG weld on carbon steel meets the same strength requirements as a TIG weld, and structural codes such as AWS D1.1 recognize both processes. TIG gives the welder more control, which helps on thin material and difficult joints, but the deciding factors for strength are procedure, fit-up and welder qualification.
Which is better for welding aluminum, MIG or TIG?
TIG on alternating current is usually better for thin aluminum sheet and cosmetic joints, because the welder can manage heat closely and the AC cycle cleans the surface oxide. MIG with a spool gun or push-pull feeder is much faster on thicker aluminum and long seams, making it the more economical choice for heavier production parts.
Why is TIG welding more expensive?
TIG is slower and more labor intensive. The welder feeds filler by hand while controlling the arc, so travel speeds and deposition rates are much lower than MIG, and the process requires more training and cleaner joint preparation. On long seams or large weldments, those labor hours make TIG noticeably more expensive per inch of weld.
What gas is used for MIG and TIG welding?
TIG welding generally uses pure argon for steel, stainless and aluminum. MIG welding on carbon steel commonly uses a blend of 75% argon and 25% carbon dioxide, while stainless MIG uses argon-rich blends designed for stainless, and aluminum MIG uses pure argon or argon mixed with helium for added heat on thick sections.
When does robotic MIG welding make sense?
Robotic MIG welding makes sense for repeat parts in production quantities with consistent component dimensions and good torch access to each joint. The robot holds speed, angle and wire position steady, giving uniform welds and high arc-on time. For prototypes, one-off weldments or very low volumes, manual welding is usually faster to set up and more economical.